Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of 6al-4v astmb381 gr5 titanium block in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
1. Gr5 titanium block is a high-strength and durable material that is commonly used in various industries. It is made up of a mixture of titanium and aluminum, which makes it stronger and more resistant to corrosion than pure titanium.
2. Ti-6al-4v Gr5 Titanium Alloy block size and standards
Size: 75x105x415mm or customer size
Standards: ASTMB381
Surface: titanium bright surface, polishing surface
Production lead time: stock 1 or 2 days, ordered 7 to 10 days, bulk order 15~30days
The block has a rectangular shape and comes in various sizes, ranging from small to large. It is commonly used in the manufacturing of aerospace components, medical implants, automotive parts, and various other applications that require high strength, durability, and corrosion resistance.


3. What is the manufacturing process of Gr5 titanium block?
Titanium ingot--Cutting--titanium square--forging--titanium block--polishing or peeling--UT test--size inspection--package--delivery

4. Gr5 titanium block according to ASTMB381 tensile strength and yield
| Grade | tensile strength | yield strength | Elongation (%) |
| F5 | 895 | 828 | 10 |
5. Gr5 titanium block advantages and features
The presence of impurities in titanium has a great impact on its mechanical properties, especially interstitial impurities (oxygen, nitrogen, carbon) can greatly improve the strength of titanium and significantly reduce its plasticity. Titanium alloys have good mechanical properties as structural materials. High strength and good processability can be achieved by strictly controlling the appropriate impurity content and adding alloy elements.
GR5 titanium block is machinable and can be readily formed into various shapes and sizes to meet specific project requirements. It is also lightweight and has a high strength-to-weight ratio, making it an ideal material in high-performance applications.

6. Why choose us?
We have years of experience in titanium from ingot to finish products, especially for export quality products, the full process cost control, and comprehensive testing system, some size Gr5 titanium blocks in stock, short delivery lead time and export quality ensure, inquiry pls send to sales@tmsalloy.com.