Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of ni200 ni201 astmb162 pure nickel foil roll in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
Products Introduction
1. Nickel foil roll is a very thin metal strip made of pure nickel and nickel alloy, which is widely used in magnetic shielding, circuit boards, transformers, batteries, electric blankets, loudspeakers, and other production fields.
2. Basic information
Grade: N4, N6, Ni201, N02200, N02201
Thickness: 5 ~ 50μm (tolerance± 5%)
Width: 0 ~ 1350mm Length: Unlimited
Supply status: soft state (M state), semi-hard state (1/4H, 1/2H, 3/4H) hard state (H state).
3. Parameters of Ni foil
Density: 8.9g/cm3
Chemical composition: nickel (purity: 99.96%)
Tensile strength: 1030rm / MPa
Elongation after fracture: 1.0 A50mm/%
Resistivity: 0.076 Ω· mm2/M
Finish: 0.15-0.25Ra
Detail Shows


4. Nickel foil roll as hot rolling or cold rolling process, it is mainly used in Ni MH batteries, lithium batteries, combined battery and power tools, communication information, special lamp, and other industries.
5. As a professional nickel foil roll supplier, we not only offer nickel 201 foil, nickel 200 foil, but also nickel alloy foil, ni foil tape, and some common use ni foil stock, contact us now for the price, and you can get quick quotations within 24hours.
6. Nickel 200 201 N4 N6 chemical elements according to standards
| Grade | Principal component≥% | Impurity content ≤ % | |||||||||||||||
| GB | Ni+Co | Cu | Si | Mn | C | Mg | S | P | Fe | Pb | Bi | As | Sb | Zn | Cd | Sn | Cr |
| N4 | 99.9 | 0.015 | 0.03 | 0.002 | 0.01 | 0.01 | 0.001 | 0.001 | 0.04 | 0.001 | 0.001 | 0.001 | 0.001 | 0.005 | 0.001 | 0.001 | |
| N5 | 99 | 0.25 | 0.3 | 0.35 | 0.02 | 0.01 | 0.4 | 0.2 | |||||||||
| N6 | 99.5 | 0.1 | 0.1 | 0.05 | 0.1 | 0.1 | 0.005 | 0.002 | 0.1 | 0.002 | 0.002 | 0.002 | 0.002 | 0.007 | 0.002 | 0.002 | |
| N7 | 99 | 0.25 | 0.3 | 0.35 | 0.15 | 0.01 | 0.4 | 0.2 | |||||||||
| Note: | |||||||||||||||||
| American standard N02201 is equivalent to the GB standard N4. | |||||||||||||||||