Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of gr2 pure titanium globe valve in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
1. Titanium Globe Valve is a kind of shunt merging or flow direction switching device, titanium globe valve adopts a top-mounted structure, which reduces the connecting bolts of the valve body itself under the conditions of high pressure and large diameter, enhances the reliability of the valve and can overcome the influence of the self-weight of the system on the normal operation of the valve.
2. Titanium Globe Valve Main Parameters:
Titanium globe valve nominal diameter: DN50mm-DN300mm;
Nominal pressure of titanium globe valve: PN1.0MPa-1.6MPa;
Titanium globe valve temperature range: -29°C-300°C.


3. Titanium Globe Valve main material
Body, Bonnet: Gr2, Gr5, Gr7, Gr12
Spheres: Gr2, Gr5, Gr7, Gr12
Seat: Gr2, Gr5, Gr7, Gr12
Stem: Gr2, Gr5, Gr7, Gr12
Seal: PTFE, RPTFE, PPL, PEEK
4. What are the applications of titanium globe valves?
Titanium globe valves are widely used in coal chemical, petrochemical, rubber, papermaking, pharmaceutical, and other pipelines as a medium of diversion and merging or flow direction switching devices.
5. What is the production process of titanium globe valve?
The titanium globe valve is one of the many types of titanium valves, and its main production process is basically the same as that of general titanium valves, mainly in the following steps.
1. The selection of materials
Titanium globe valve is a high-strength, corrosion-resistant valve, and the choice of material is very critical. The first thing is to choose high-quality raw materials to ensure the purity and quality of the materials. Secondly, according to the specific use environment and work requirements, choose the appropriate titanium alloy materials, such as Gr1, Gr2, Gr5, Gr7, etc.
2. Smelting
The melting of titanium alloy is the first and most critical step in valve pouring. In the melting process, the furnace temperature, melt temperature and melt composition should be controlled to ensure the purity and uniformity of the melt. At the same time, it is also necessary to pay attention to the oxidation problem in the smelting process and take corresponding measures to reduce the degree of oxidation.

3. Pouring
During the pouring process, it is necessary to pay attention to the structure and shape of the valve to ensure that the poured metal fills the entire mold to avoid bubbles and defects. In addition, it is necessary to pay attention to the temperature and speed at the time of pouring to ensure that the pouring is sufficient and uniform.
4. Cooling
After the valve is poured, it is cooled. During the cooling process, care should be taken to avoid rapid temperature changes to avoid cracks and deformation of the valves. At the same time, it is necessary to carry out proper annealing treatment to improve the strength and corrosion resistance of the valve.
FAQ
Q: 1. What is the maximum temperature that can be used with a titanium globe valve?
A: The maximum temperature that titanium valves can use is 300°C The nominal pressure range of the titanium valve is PN1.0MPa-1.6MPa, and the temperature range is -29°C-300°C
Q: 2. What are the advantages of titanium globe valves?
A: Titanium globe valve, a valve made of titanium material. In a highly corrosive environment, the oxide film has good stability and self-passivation ability, which is a characteristic to resist strong corrosion under a variety of harsh working conditions.
Q: 3. Is the titanium globe valve in stock?
A: Some specifications of titanium globe valve are in stock, and more specifications can be customized, and the customized construction period is 15~20 days.
Q: 4. What is the MOQ of the titanium globe valve?
A: Titanium globe valve stock specification MOQ1~2 pieces, customized specifications from 5~10 pieces.
Contact information:
Tel: +86-0917- 3664600
Whatsapp: +8618791798690
Email: sales@tmsalloy.com
tina@tmsalloy.com
Hot Tags: gr2 pure titanium globe valve, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Titanium Alloy Valve