The iridium-tantalum anode rod is a high-performance electrochemical electrode with a titanium-based substrate and an iridium-tantalum oxide (IrO₂-Ta₂O₅) composite coating on its surface. It features excellent catalytic activity, corrosion resistance, and long service life, making it widely used in industrial applications such as hydrogen production through water electrolysis, electroplating, and wastewater treatment.
Core Structure and Principles
Substrate: A first-grade pure titanium (TA1) is used as the supporting body, providing excellent mechanical strength and conductivity.
Coating: The surface is coated with iridium oxide and tantalum oxide via thermal decomposition, where:
IrO₂ provides highly efficient oxygen evolution reaction (OER) catalytic activity, reducing electrolysis energy consumption;
Ta₂O₅ enhances coating stability, inhibits grain growth, prevents titanium matrix oxidation, and extends service life.
Synergistic effect: Forms a "active-stable" dual-core structure, enabling stable operation in acidic, alkaline, and chlorine-containing environments.

Specification Tel:0917-3664600
| Grade | Gr1 Gr2 titanium |
| Size | According to the customer's size |
| Coating | Iridium tantalum coating 4um |
| Standards | ASTM B348 |
Product Pictures Tel:0917-3664600



Advantages of iridium coated tantalum anode rod Tel:0917-3664600
Key Performance Advantages
1.extraordinary longevity
Under the conditions of a 20% sulfuric acid solution and 5kA/m², the lifespan can exceed 2 years, surpassing that of traditional graphite anodes by more than 10 times.
2.Low energy consumption
In hydrogen production through water electrolysis, the cell voltage is reduced by 0.3–0.5V compared to nickel-based anodes, enabling annual power savings of up to 4 million kWh in megawatt-scale projects.
3.High current density adaptability
Supports operation at 10–50A/dm², suitable for high-current-density scenarios such as copper foil production, with a production efficiency improvement of over 30%.
4.Strong environmental adaptability
Resistant to chloride corrosion (≤200g/L), high temperature (≤80°C), and pH fluctuations (2–14), suitable for complex working conditions such as seawater desalination and chlorinated wastewater treatment.
Applications of iridium tantalum anode rod
Ir-Ta anode rods find applications in various industries, including chlor-alkali production, electrolysis, electroplating, water treatment, and more. They are particularly well-suited for demanding environments where corrosion resistance, mechanical strength, and long-term stability are required.
- Chlor-Alkali Industry: Ir-Ta anode rods are extensively used in the chlor-alkali industry for the production of chlorine, sodium hydroxide, and other alkali products. They withstand the highly corrosive environment of electrolytic cells and ensure efficient and reliable electrolysis.
- Electroplating: Ir-Ta anode-coated titanium anode rods are employed in electroplating processes to deposit a wide range of metals onto a substrate. Their excellent corrosion resistance and uniform current distribution help achieve high-quality, uniform plating results.
- Electrowinning: Ir-Ta anode rods are suitable for electrowinning processes, where metals are extracted from solutions or ores through electrolysis. They provide long-lasting performance and withstand corrosive environments, ensuring effective metal recovery.
- Water Treatment: Ir-Ta anode bars are utilized in electrochemical water treatment systems for disinfection, oxidation, and other purification processes. Their corrosion resistance and stability contribute to the efficient removal of contaminants and pathogens.
- Electrosynthesis: Ir-Ta-coated titanium anode rods are employed in various electrosynthetic reactions, including organic synthesis and electro-oxidation processes. They provide a stable and durable electrode surface, enabling efficient conversion of reactants.
Pacakge and delivery
Package and delivery have become essential aspects of modern-day commerce. With the rise of e-commerce, online shopping has become increasingly popular, and package and delivery services have become a crucial component of the supply chain.
Package and delivery refer to the process of transporting goods from one place to another through various means such as postal services, courier companies, and logistics providers. The primary objective of package and delivery is to ensure that the goods are delivered to their intended recipients in a timely, safe, and efficient manner.
The package and delivery process starts with the sender preparing the package for shipment by packaging the goods securely and labeling them correctly. The package is then handed over to the delivery company, which arranges for the transportation of the package to its destination.
Various modes of transportation are used for packaging and delivery, including land, air, and sea. The mode of transportation used depends on various factors such as the distance between the sender and recipient, the size and weight of the package, and the urgency of delivery.

When considering buying Ir-Ta anode rods, it is important to evaluate specific application requirements and consult our engineers, based on specific requirements and conditions, they can provide you with more accurate advice and choose suitable products. They can provide additional insights and help determine whether Ir-Ta anode rods are the best choice for your particular application.
Contact Us
No.11th Road of Gaoxin, Baoji, Shaanxi, P.R.China
Tel: +86-0917- 3664600
Fax: +86-0917- 3664600
Whatsapp: +8618791798690
Mail: sales@tmsalloy.com
Other related MMO titanium anodes.

Hot Tags: iridium tantalum anode rod, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, MMO Ruthenium Iridium Coated Titanium Anode Rod, MMO Titanium Anode Titanium Mesh Electrode, Iridium Coated Titanium Anode Mesh, Platinum Coated Titanium Plates Platinized Titanium Anode, Iridium Tantalum Anode Rod, Ruthenium Iridium Titanium Anode Plate