Moly Wire Molybdenum Wire for EDM Wire Cutting Machine 0.18 mm

Moly Wire Molybdenum Wire for EDM Wire Cutting Machine 0.18 mm

Moly wire
Molybdenum wire price
Molybdenum wire mesh
Send Inquiry
Chat Now
Description

Providing customers with high-quality, safe and reliable Titanium Grade 4 Bars, Gr2 Titanium Round Bar, titanium clad copper rod is our eternal foothold in the market. We've been looking forward to your inquiry and order. We continue to shape the iconic image of the company, highlighting our unique culture and characteristics. We've got always been in line with serving customers, creating value management objectives and adhering to the sincerity, dedication, persistent management idea.

Products Introduction

1. Molybdenum wire, often known as Moly Wire, is a refractory metal that melts at 4760°F.

2. Basic information

The forming process of molybdenum wires surface state: drawing, forging, and polishing

Features of moly Wire

① Molybdenum wire has high precision, and the wire diameter tolerance is controlled within 0 ~ - 0.002mm;

② Low wire breakage rate, high processing speed, and high-cost performance;

③ It can realize stable long-time continuous processing.

Molybdenum wire employs modern hot and cold drawing combination technology to form high-quality, high-temperature molybdenum raw materials into a linear shape and then uses them as electrodes on wire-cutting machines to process the workpiece.

Detail Shows

molybdenum wire

Molybdenum wire

molybdenum wire price

3. Chemical composition of molybdenum wire

GradeMo purity%other elements≤%Each element≤%Element content append%
Mo199.950.050.01/
Mo299.90.10.01/
Mo399.330.070.010.2-0.6
Gradedescriptionapplications
MO1pure moly wireIt is used in the manufacture of electronic vacuum devices, thermal components, heating elements, different types of bulb hooks, mandrel crimped tungsten wires, etc
For wire cutting
MO2pure moly rodUsed in the manufacture of electronic vacuum devices, electrode gas discharge tubes, lamps, and electronic tube supports.
MO3molybdenum with other elementsHigh-temperature structural materials (printer needle, nut, screw), halogen lamp support, heating wire, and the radial axis of the tube.

4. Moly wires applications:

1. Hot Zones for high-temperature furnaces.

2. Sputtering targets for coating solar cells & flat screens.

3. Glass melting electrodes

4. Heat shields

5. Semiconductor base plates.

6. Brazing fixtures & Boring bars

7. Pigments and catalysts.

5. The manufacturing process of molybdenum wire

Molybdenum wire mainly refers to a consumable made of precious metals such as molybdenum, which is continuously moved with a high-voltage electric field to cut the workpiece during wire cutting. Molybdenum wire has been widely employed as an important metal material in aircraft, the metallurgical chemical industry, mechanical electronics, vehicle manufacture, and other sectors. The production process of molybdenum wire is as follows:

Molybdenum wire is made of metal molybdenum powder as raw material. After obtaining square or round bar-shaped metal molybdenum by powder metallurgy, it is made by rolling, rotary forging, stretching, and other pressure processing and supplemented by various technological means. Finished wire of different varieties and specifications (generally d6.5~0.02mm, and mainly d3.5~0.05mm).

buy Molybdenum Wire price

The Moly Wire Molybdenum Wire for EDM Wire Cutting Machine 0.18 mm produced by the company enjoys a good reputation in our industry and customer groups. After years' creating and developing, with the advantages of trained qualified talents and rich marketing experience, outstanding achievements were gradually made. All of our products are produced in strict accordance with the technological process, and have reached advanced technology and high quality, ensuring that the qualified rate of products reaches 100%.

Hot Tags: molybdenum wire, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Tantalum Ta Sputtering Targets, titanium strip stock, ASTM B363 wpt2 Elbow, platinum titanium electrode, Titanium Grade 2 hex bolts, titanium fittings;