To create more value for Titanium Wire Mesh, Titanium Clad Steel Plate, Titanium. Our manufacturing equipment, test and detection means have reached and approached the international advanced level, and our competitiveness has been continuously improved. Facing the future, we unswervingly take the road of sustainable ecological environment and sustainable development of resource development. Adhering to the principle of honest management and customer first, we have been providing users with good products and satisfactory services.

Products Introduction

1. Zirconium bar is a metal solid bar that is made of zirconium, it is widely used in various anticorrosive agitator shafts, crucibles, and screws.

2. Zirconium bar basic information

Size: 5.0~120mm

Length 50-3000mm for bars, or any length the customer desires

Standards: ASTM B550

Zirconium bar Physical Properties
MaterialStateRm(≥)/MPaRp0.2(PaA50mm(≥)/%
Zirconium 702annealed37920716
Zirconium 704annealed41324114
Zirconium 705annealed55237916

Detail Shows

zirconium bar

zirconium bar stock

3. Zirconium bar can be an ideal raw material for other shapes such as agitator shafts, and crucibles. Zirconium rods are also used for zirconium electrodes.

Zirconium

Method for preparing metal zirconium

A method for preparing zirconium sponge by reducing zirconium tetrachloride (ZrCl4) with metal magnesium. It mainly includes 3steps.

Decomposition of zircon sand and preparation of zirconium tetrachloride;

Separation of zirconium and hafnium;

Zirconium tetrachloride is refined and magnesium is thermally reduced to prepare a zirconium sponge.

4. The production process of metal zirconium rods:

Zirconium ore is selected to extract zirconium ore (concentrate) and then smelted into sponge zirconium. Zirconium and hafnium are separated while the zirconium sponge is smelted to produce a hafnium sponge. Then the sponge zirconium is melted and cast into zirconium ingots, and the zirconium ingots are processed into zirconium billets (zirconium rod billets, etc.), and finally subjected to pressure processing such as extrusion into zirconium bar.

5. Our advantages

Zirconium bars are the starting point of many deep-processing zirconium products. Our free forging equipment can uniformly deform zirconium ingots from the inside to the outside in a short period of time during the forging process, destroying the grain structure and improving the mechanical properties of zirconium materials.

Compared with hammer forging, the material quality has been greatly improved, after several times of rolling and annealing, a smaller diameter can be obtained, and finally, the oxide layer on the surface is removed by machining, we can provide zirconium 702 bars with turned and polished surfaces.

We rely on integrated large-scale manufacturing capabilities and advanced management concepts to provide customers with high quality Cheap Price X-ray Filter Zirconium Bar for Industrial Use. We are willing to provide users with all-round, diversified and wide-ranging services, and sincerely cooperate with colleagues from all walks of life to create brilliance. We always pursue the goal of globalization, and maintain and provide high-quality customer service to our dealers and end customers all over the world as our necessary business philosophy.

Hot Tags: zirconium bar, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Gr1 Titanium Plate, Titanium Products, Titanium Nuts, Tungsten Plate, Nickel Crucible, Gr5 Titanium Screw

You May Also Like
Send Inquiry