Our 6al4v titanium plate, nickel wire resistence, molybdenum round bar has won the favor of consumers at home and abroad by virtue of its excellent cost performance. Its quality is stable and durable. We have always been in line with: sincere hospitality, customer first service purpose, has been the majority of customers praise. The enterprise will take "enthusiastic service, professional production, affordable price" as the concept.
Products Introduction
1. Zirconium wires are a special form of silver-white metal wire that is a rare metal. It is mainly used for welding chemical corrosion-resistant structural parts.
2. Specifications of Zirconium Wire
Material ERZr2, ERZr3, ERZr4, high purity zirconium
Size 0.3-6.0mm diameter x L
Zirconium wires specification ASTM B550/550M-07, AWS A5.24
Supplied as in rolls, straight wire, on the spool
3. Features of zirconium wire
It presents the appearance of silver metal, like most zirconium products. Zirconium wires have a high melting point of 1855 ° C and a small neutron absorption cross-section, which is very suitable for the nuclear power industry. Zirconium wire also has many other applications as people are becoming more familiar with the product.
Detail Shows

Zirconium welding wire

Zirconium tig wire
4. How is the zirconium wire made?
Zirconium is a hard, glossy, silvery-colored metal that is extracted from its ores (the oxide or zircon, ZrSiO4) by converting it to a tetrahalide and then reducing it with magnesium. The metal has strong corrosion resistance and is not affected by acids (except HF) and alkalis due to the stable oxide film of the surface.
5. Zirconium wires applications
It is mainly used to weld chemical equipment in acetic acid production, including heat exchangers, condensers, strippers, reaction vessels, pumps, valves, and pipelines. The corrosion resistance of zirconium can greatly prolong the service life of equipment and pipelines, reduce maintenance costs, and minimize production shutdown time.
The melting point of zirconium wires is higher than that of titanium, the density is higher than that of titanium, and the specific heat is smaller than that of titanium. As a result, the heat input required for welding is a little higher than for titanium.
Zirconium has a much lower expansion coefficient than other materials, and it is smaller than that titanium. Welding is made possible by the minor deformation and decreased tension that occurs during welding.
Numerous welding techniques can be utilized as zirconium has a low tendency to break during welding, and argon arc welding is one of the more affordable ones. The key is protection.
6. Why choose us
Our zirconium wires are made of high-quality raw materials and can be customized according to customer requirements, fast delivery, good quality, zirconium welding wire, and zirconium wire on spool, some specifications are available in stock, the pursuit of continuous improvement of efficiency is our long-term goal, and ultimately achieving the price vs performance ratio of the product.
7. FAQ
Production lead time: customized delivery within 10~15 working days
Payment method: 30% prepaid, the rest paid before delivery
Delivery method: send to the customer's destinations or seaport and airport.
Packing: Standard export wooden box packing
Our company's goal is to develop new markets or regions and accelerate the launch of new Gh4648 Nickel Wire for High Temperature Structure Parts or services. With high quality, reasonable price, on-time delivery and customized & customized services to help customers achieve their goals successfully, our company has got praise in both domestic and foreign markets. We are committed to the common development of employees and the company, and hope that the company's achievements in development will benefit employees, and employees will realize their self-worth in development.
Hot Tags: zirconium wires, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, titanium sheet stock, ERTi 1 AWS A5 16, titanium v stakes, zirconium welding wire, 6-6-2 titanium, ni foil