ASTM F136 Medical Titanium Bar/Titanium Alloy Bar for Orthopedics

ASTM F136 Medical Titanium Bar/Titanium Alloy Bar for Orthopedics

titanium bar for medical use
Titanium bar for medical implant
gr5 Medical titanium bar
titanium bar ASTM F136
TA6V ELI grade
Medical grade 5 ASTM F136
Gr.5 medical implant Titanium rod
Send Inquiry
Chat Now
Description

We are a professional manufacturer for vessel dished ends, inconel bar, head of pressure vessel, with a complete and scientific quality management system. Our enterprise spirit is that unity makes dreams come true and diligence creates excellence. Our company always adheres to the business philosophy of sincerity and quality, and insists on the management philosophy of people-oriented and efficient cooperation.

Products Introduction

1. Medical titanium bar is a metal solid bar used for medical implants or medical devices, such as artificial joints, bone plates, screws, and surgical instruments.

2. What is the grade of the medical titanium bar?

Pure titanium: Gr1 Gr4

Titanium alloy: Gr23 Gr5ELI (TA6V ELI)

3. Standards of titanium bar for medical use:

ASTM F136 for titanium alloy

ASTMF67 for pure titanium

4. Chemical elements and Mechanical Properties according to ASTMF136

ElementComposition,%
Nitrogen, max0.05
Carbon, max0.08
Hydrogen, max0.012
Iron, max0.25
Oxygen, max0.13
Aluminum5.5-6.50
Vanadium3.5-4.5
Titaniumbalance
Nominal Diameter or DistanceTensile Strength min,Yield Strength
m
ElongationReduction
Between Parallel Sides, in. (mm)psi(MPa)(0.2% offset Min,psi(MPa)LL
Under 0.187 (4.75) thickness or diameter86079510---
0.187(4.75) to under 1.75(44.45),incl8607951025
1.75 (44.45) to under 2.50(63.50),incl825760820
2.50(63.50) to 4.00(101.60),incl825760815

titanium bar for medical use

5. What are the advantages of medical titanium bar?

Medical titanium rods have low density, are lightweight, have high strength, have good biocompatibility with the human body, and the material is corrosion-resistant in the human environment.

6. Our advantages

We have complete processing equipment and rich processing experience. The medical titanium rods all have been tested by a third party (chemical composition, mechanical properties, metallographic structure, tolerance), polished and polished rods have undergone flaw detection treatment and the product quality stabilize. it is mainly used in machinery equipment, electroplating equipment, medical, various precision parts, and other industries.

gr5 Medical titanium bar

7. Other related titanium bars for medical applications

Medical titanium bars are widely used in the medical industry due to their high biocompatibility and corrosion resistance. These bars are made from pure titanium or titanium alloys such as Ti-6Al-4V, Ti-6Al-7Nb, and Ti-13Nb-13Zr, among others. The following are some product descriptions of medical titanium bars:

Pure Titanium Bar: It is a medical-grade titanium bar that is 99.5% pure. Pure titanium bars are used in surgical implants, dental implants, and other medical devices.

Ti-6Al-4V Bar: This is the most commonly used titanium alloy for medical implants because it is lightweight, strong, and biocompatible. It is used in the manufacture of orthopedic implants, bone screws, dental implants, and spinal fixation devices.

Ti-6Al-7Nb Bar: This alloy has excellent biocompatibility, making it ideal for medical implants such as artificial knee and hip joints. Its high strength and corrosion resistance also make it a popular choice for dental implants.

Ti-13Nb-13Zr Bar: This alloy is often used in the manufacture of orthopedic implants and dental implants. It has a low modulus of elasticity, which reduces stress on the surrounding bone tissue.

Medical titanium bars are essential components in the manufacturing of medical devices and implants. They offer exceptional biocompatibility, corrosion resistance, and strength, making them ideal for use in the human body.

For technology, we tirelessly pursue breakthroughs, put customer needs first, and strive to develop new ASTM F136 Medical Titanium Bar/Titanium Alloy Bar for Orthopedics. We take "respecting harmony and keeping promise" as the fundamental of enterprise development. While striving to improve ourselves, we also further strengthen the company's comprehensive competitiveness. We put the needs of our customers first, and look forward to business negotiations with new and old customers.

Hot Tags: ASTM F136/F67 Medical Titanium Bar, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, hemispherical head pressure vessel, Gr5 Titanium Plate, Buy molybdenum nut, nickel fittings, titanium spring wire, 1 kilo titanium bar

You May Also Like
Send Inquiry