Custom Sheet Metal Laser Letters Cutting Parts Custom Production Metal Fabrication Customized Laser Cutting Solutions Sheet Metal Laser Cutting

Custom Sheet Metal Laser Letters Cutting Parts Custom Production Metal Fabrication Customized Laser Cutting Solutions Sheet Metal Laser Cutting

cutting titanium with lasers
Laser Cut Titanium Grade 5
Titanium Sheet Cutting - Laser vs Water
Titanium CNC Laser Cutting
Send Inquiry
Chat Now
Description

In line with the concept of integrity, innovation, transcendence, and efficiency, while providing first-class ti bicycle bolts titanium screws for bicycles, tube titanium, t25 titanium bolts, we also clarify our social responsibilities and pay more attention to the interests of customers. We have a sense of social responsibility, abide by the law and discipline, protect the environment, and pursue the harmony between enterprise growth and social development. Survive by quality and development by reputation are our company's business philosophy. We will do our best to do a good job in products and services in order to improve the confidence of our new and old customers. Looking forward to the future, all colleagues of our company will always adhere to the enterprise spirit of dedication and love, reform and innovation, and work hand in hand with the majority of users to create a brilliant tomorrow. We continue to establish and improve the standard management system, strengthen the construction of incentive mechanism and enhance the cohesion of the company.

Products Introduction

1. laser cutting titanium sheet is the sheet metal that is cut by laser beam a thermal cutting method, it is an advanced and widely used cutting process.

Laser cutting is beneficial for cutting titanium sheets due to its high strength and durability, making it a popular material in aerospace, medical, and other high-performance industries. The process can cut titanium sheets up to 6mm in thickness and can produce complex shapes and patterns without the need for extensive tooling.

2. What is laser cutting?

laser cutting uses a high-power density beam to irradiate the material to be cut, the material is quickly heated to the vaporization temperature and evaporated to form holes. As the beam moves to the material, the holes continuously form slits with a narrow width (such as about 0.1mm), to complete the cutting of the material.

3. What is the titanium sheet's material grade for laser cutting?

Grade: Gr1 Gr2 Gr3 Gr4 Gr5 Gr6 Gr7 Gr12 etc.

When laser cutting titanium sheets, the process can be optimized based on the specific grade of titanium being used. For example, some grades require higher laser power, while others are more sensitive to heat and may require slower cutting speeds. The process also requires careful preparation to prevent oxidation, which can affect the quality of the cut.

Detail Shows

Titanium Sheet Cutting - Laser vs Water
Titanium CNC Laser Cutting

4. How to cut the titanium sheet with a laser beam?

The titanium plate is cut with argon and nitrogen as a processing gas. So how do you use a laser to cut a titanium plate? Methods and steps of laser cutting titanium plate:

1) Place the titanium alloy steel plate after surface treatment on the cutting platform to prepare for cutting:

2) Move the laser nozzle with a diameter of 2m to the extension line of the cutting line. At this time, the distance between the laser nozzle and the starting point of the cutting line is 50cm. Adjust the height of the laser nozzle and keep the distance between the laser nozzle and the titanium alloy steel plate at 0.7mm;

3) Adjust the penetration air pressure to 2.5bar and the cutting air pressure to 1bar to prepare for cutting;

4) Turn on the motor to drive the laser nozzle to move at a uniform speed to the starting point of the cutting line at a speed of 450m / min. no laser is emitted at this stage

5) When the laser nozzle maintains the moving speed in step 4) to the starting point of the cutting line, emit the laser and start cutting. At this time, the cutting speed is 4-5m / min

6) After the laser nozzle moves past the end position of the cutting line, that is, Turn off the laser emission when the cutting is finished, and stop when the laser nozzle has moved for 30 cm. The width of the notch is 0.11M, and the two sides of the cutting seam are parallel and have good perpendicularity with the surface. The dimensional accuracy of the cutting parts is high, and the positioning accuracy is 0.04mm.

Laser Cut Titanium (Grade 5)
cutting titanium with lasers (3)

5. What are the advantages of laser cutting titanium sheets?

  1. Laser cutting is suitable for the production of small batches of various sizes of parts because there is no tooling cost, these parts were not available before, titanium plates, which may be used to produce a variety of parts at the trial stage, can be laser cut with no MOQ restriction.

  2. Lasers can precisely and efficiently cut titanium, and when using nitrogen protection, the laser cutting tolerance can reach 0.1mm.

  3. Laser cutting adopts computer numerical control technology (CNC) equipment. This device can receive cutting data from a computer-aided design (CAD) workstation. So the titanium plate can be processed into various complex cutting parts, as long as we get your drawings.

6. Why choose us

Our professionals at Laser are trained to work with this rigid metal to give you the smoothest lines with minimal tolerance levels for the most complex or the simplest projects that you may have.

Titanium laser cutting parts are available for construction, railways, equipment, instruments, and medical device。

7. Where to buy the titanium sheet with laser cutting?

Call us right away at 917-466-4600 or email sales@tmsalloy.com with any questions you may have regarding a project, and we'll be happy to respond with lead times, estimates, and more. Get in touch today to discuss your project.

We continue to innovate according to the needs of our customers, conduct transparent cooperation with our partners, and provide customers with the best comprehensive solutions and services in the field of Custom Sheet Metal Laser Letters Cutting Parts Custom Production Metal Fabrication Customized Laser Cutting Solutions Sheet Metal Laser Cutting. With the strong position of market demanders, customer response time has become the main concern of our company. We have always been committed to building up the competitiveness of our company, and insisting on customer-centric, providing customers with high-quality pre-sales and after-sales services, delivery time, and timely feedback.

Hot Tags: laser cutting titanium sheet, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, zirconium tube material, Zirconium Crucible, tantalum round bar, ti screw, Gr2 Titanium Screw, TA6V ELI grade

You May Also Like
Send Inquiry