Our new Nickel Products, Zirconium screw price, Gr2 Titanium Sheet have the ability of low cost and rapid response to the market, which is the key to our rapid development and market share. The creation of international brands is our never-ending pursuit of the goal. Enterprises must follow the law of development and the law of talent growth; employees must be loyal to their own roles, dedicated to their jobs, and keep their duties in order to become a company for everyone. We not only want to meet the needs of our customers, but also to exceed their expectations and achieve the economic and social benefits of our company simultaneously.
1. Products Introduction
A titanium square bar is a rectangular bar made of titanium and titanium alloy, also known as titanium square rods. It has a small density (4.51), is lightweight, and has good thermal stability.
2. Basic information
Grade: Gr2 Gr5 Gr7
Size: 8x8mm, 10X10mm, 12X12mm
Standards: ASTMB348
3. Titanium square rod features:
Strong corrosion resistance, acid, and alkali corrosion resistance. Seawater corrosion resistance and sewage corrosion resistance.
Between - 253-600 °, the tensile strength of titanium is almost high in metals.
Nonmagnetic, small coefficient of linear expansion.
Titanium products have low density and high specific strength: good corrosion resistance and heat resistance. The new titanium alloy rod can be used for a long time at 600 ℃ or higher temperature, with low-temperature resistance.
Detail Shows


4. Titanium metal bar tensile yield and elongation according to ASTMB348
Grade | Tensile Strength | Yield Strength | Elongation in 4D, min, % | Reduction of Area, min % |
Gr2 | 345 | 275 | 20 | 30 |
Gr5 | 895 | 828 | 10 | 25 |
Gr7 | 345 | 275 | 20 | 30 |
5. Applications of titanium square bar
Titanium square bars are widely used in the electroplating industry and the production of hangers and pendants for metal pickling treatment.
The main specifications are 6*6mm 8*8mm 10*10mm 12*12mm 14*14mm etc, other specifications also can be ordered according to the customer's request.
Chemical processing - Titanium square bars are resistant to corrosion by most chemicals, making them ideal for use in chemical processing plants.
Sports equipment - Titanium square bars are used in the manufacture of sports equipment such as golf clubs, tennis rackets, and bike frames due to their strength and lightweight properties.
Automotive industry - Titanium square bars are used in the automotive industry in the manufacture of engine components, exhaust systems, and suspension systems due to their high strength and resistance to corrosion.
Marine industry - Titanium square bars are used in the marine industry for boat and shipbuilding due to their resistance to corrosion and high strength.
6. Our advantages
As a professional titanium bar supplier, we can not only supply titanium square bars, and titanium angle bars but also offer various titanium metal rods, which include pure titanium bars (Gr1 Gr2 Gr3 Gr4), titanium alloy bars (Gr5 Gr6 Gr7 Gr9 Gr12 Gr23) and other titanium bars CNC machining parts according to drawings. Contact us to get the titanium bar price per kg by mail now at sales@tmsalloy.com
7. Some common use titanium bar stock list
Pure titanium | Titanium alloy | |||||||
Grade | Size (mm) | weight (kg) | Grade | Size (mm) | weight (kg) | Grade | Size (mm) | weight (kg) |
Gr2 | φ4 | 100 | Gr1 | φ4 | 150 | Gr5 | φ20 | 100 |
Gr2 | φ5 | 120 | Gr1 | φ5 | 150 | Gr5 | φ25 | 100 |
Gr2 | φ6 | 110 | Gr1 | φ6 | 150 | Gr5 | φ27 | 100 |
Gr2 | φ7 | 100 | Gr1 | φ7 | 150 | Gr5 | φ28 | 30 |
Gr2 | φ8 | 100 | Gr1 | φ8 | 150 | Gr5 | φ29 | 120 |
Gr2 | φ9 | 150 | Gr1 | φ9 | 150 | Gr5 | φ30 | 300 |
Gr2 | φ10 | 130 | Gr1 | φ10 | 150 | Gr5 | φ32 | 300 |
Gr2 | φ15 | 200 | Gr1 | φ15 | 150 | Gr5 | φ35 | 280 |
Gr2 | φ16 | 80 | Gr1 | φ16 | 150 | Gr5 | φ38 | 170 |
Gr2 | φ17 | 95 | Gr1 | φ17 | 150 | Gr5 | φ40 | 150 |
Gr2 | φ18 | 160 | Gr1 | φ18 | 150 | Gr5 | φ45 | 300 |
Gr2 | φ18.8 | 150 | Gr1 | φ18.8 | 150 | Gr5 | φ48 | 300 |
Gr2 | φ19 | 200 | Gr1 | φ19 | 150 | Gr5 | φ50 | 300 |
Gr2 | φ20 | 300 | Gr1 | φ20 | 150 | Gr5 | φ55 | 160 |
Gr2 | φ25 | 300 | Gr1 | φ25 | 200 | Gr5 | φ60 | 100 |
Gr2 | φ26 | 300 | Gr1 | φ26 | 200 | Gr5 | φ65 | 100 |
Gr2 | φ27 | 300 | Gr1 | φ27 | 200 | Gr5 | φ67 | 70 |
Gr2 | φ28 | 300 | Gr1 | φ28 | 200 | Gr5 | φ70 | 180 |
Gr2 | φ30 | 300 | Gr1 | φ30 | 200 | Gr5 | φ75 | 120 |
Gr2 | φ31 | 300 | Gr1 | φ31 | 200 | Gr5 | φ80 | 200 |
Gr2 | φ32 | 300 | Gr1 | φ32 | 200 | Gr5 | φ82 | 50 |
Gr2 | φ33 | 300 | Gr1 | φ33 | 200 | Gr5 | φ85 | 100 |
Gr2 | φ35 | 300 | Gr1 | φ35 | 200 | Gr5 | φ90 | 200 |
Gr2 | φ36 | 300 | Gr1 | φ36 | 200 | Gr5 | φ92 | 50 |
Gr2 | φ37 | 300 | Gr1 | φ37 | 200 | Gr5 | φ95 | 160 |
Gr2 | φ38 | 300 | Gr1 | φ38 | 200 | Gr5 | φ100 | 100 |
Gr2 | φ39 | 300 | Gr1 | φ39 | 200 | Gr7 | some size stock | |
Gr2 | φ40 | 300 | Gr1 | φ40 | 200 | Gr9 | some size stock | |
Gr2 | φ41 | 300 | Gr1 | φ41 | 300 | Gr12 | some size stock | |
Gr2 | φ42 | 300 | Gr1 | φ42 | 300 | specifications>φ65mm can be ordered according to the required length | ||
Gr2 | φ43 | 300 | Gr1 | φ43 | 300 | |||
Gr2 | φ44 | 300 | Gr1 | φ44 | 300 | |||
Gr2 | φ45 | 300 | Gr1 | φ45 | 300 | |||
Gr2 | φ46 | 300 | Gr1 | φ46 | 300 | |||
Gr2 | φ48 | 300 | Gr1 | φ48 | 300 | |||
Gr2 | φ50 | 300 | Gr1 | φ50 | 300 | |||
Gr2 | φ52 | 300 | Gr1 | φ52 | 300 | |||
Gr2 | φ54 | 300 | Gr1 | φ54 | 300 | |||
Gr2 | φ55 | 300 | Gr1 | φ55 | 300 | |||
Gr2 | φ60 | 300 | Gr1 | φ60 | 300 | |||
Gr2 | φ65 | 300 | Gr1 | φ65 | 300 |
Our company adopts advanced technological process and correct technical operation to develop high-quality 10mm Gr5 Eli Medical Titanium Rod for Dental Implant. We firmly believe that aggressiveness is the inexhaustible driving force of the company's operation, and high efficiency is the way of survival of the company's operation. We are willing to make friends with people from all walks of life and work together for common development and opening up new fields!
Hot Tags: ASTMB348 Grade 2 UNS R50400 Titanium Square Bar, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Titanium Sheet Cutting Laser vs Water, tantalum round bar, thin flat titanium foil titanium foil in coil, concentric titanium reducer, Gr2 Titanium Sheet, molybdenum flat bar