Home > News > Content

Zr702 Zirconium Tube

Feb 25, 2023

Basic Info.

Model NO. Zr702
Thickness Range 0.3mm-10mm
Length Range ≥500mm
Width Range 300mm-3000mm
Standard1 GB/T21183-2007
Grade1 Zr702
Material Zirconium and Other Metal
Surface Pickling Polishing
Transport Package PE Foam and Wooden Cases
Specification Thickness Range 0.3mm-10mm
Origin. Baoji China
HS Code 8109910010
Production Capacity
4500 Tons Per Year

Zr702 Seamless Tubes

Zirconium tubes are made by combining cold rolling and cold drawing processes with various alloys, most commonly zirconium, and hafnium alloys, zirconium and niobium alloys, and zirconium and titanium alloys. The most common type of zirconium tube is seamless, which is made of extruded rods and stretched through hot and cold rolling.

Zirconium tube has excellent oxidation, corrosion, and wear resistance. Because of its corrosion resistance, zirconium tube is appealing in chemical processing equipment.

Zirconium tubes are also used in the medical industry due to their biocompatibility and high strength. It is used in orthopedic tools such as drills and saws, as well as implants.