Home > News > Content

Nickel Content Of Future Garden

Feb 09, 2022

It is a forest of the future, where exquisite architecture and technological innovation are combined. "Future garden", located in Nanjing, China, is one of the scenic spots of the Jiangsu Garden Expo. 42 stainless steel trees form umbrella support for the roof. The shape of each tree is neat and connected with each other. The lotus leaf roof adopts acrylic panels, which is the first time in the world. "Future garden" is transformed from mined mines and abandoned cement plants. Although the ground conditions are complex and the construction is difficult, the completed garden is pleasing to the eye. The project uses 1000 tons of nickel-containing 316L (UNS s31603) stainless steel.