Basic Info
Model NO. W-1, W-2
Name Tungsten Bar
Usage Industrial
Market Global
Size Diameter:25mm*120mm
Transport Package Foam Wooden Box
HS Code 8101100010
Product Description
The tungsten bar is divided into sintered, forged, and spinning forged according to processing, while black,lathe-polishing, and polishing according to its surface. Since the melting point of tungsten is high, the forging tungsten stick of high purity, high density, and outstanding high-temperature creep resistance is extensively applied in making supporting tungsten crucible of sapphire growth furnace, the electrode of rare earth high-temperature furnace, heating parts, connecting parts and supporting stick. While the tungsten rod is used in making heating parts, motor contactors, and electrodes of high-power lamps whose processing methods include sintering, forging, turning to forge, and polishing.
A: For tungsten wire, the diameter is from 0.008mm~3.2mm.
For the tungsten rod, the diameter is from 2mm~100mm, length is from 50mm~2000mm.
For the tungsten sheet, the thickness is from 0.025mm~2mm, the width is from 50mm~500mm, and the max length is 1000 mm.
For the tungsten plate, the thickness is from 2.1~25mm, the width is from 30mm~600mm, and the max length is 1000mm.
For a tungsten boat, the thickness is from 0.2mm~0.5mm, the width is from 5mm~25mm, and the max length is 1000mm.
For the tungsten tube, the diameter is from 25mm~340mm, and the max length is 650mm.
For the tungsten crucible, the diameter is from 10mm~500mm, the height is from 10mm~750mm, and the thickness is from 2mm~20mm.
Q: what is the surface of your tungsten products?
A: For tungsten wire, we have a graphite black surface, an alkali cleaning surface, and an electric polished surface.
For tungsten rod&sheet&plate&boat&tube&crucible,etc
Tungsten rods, available in several sizes, are useful in a variety of applications, such as jewelry making and fine drilling. Tungsten rods offer great strength and hardness and remain stable at high temperatures. They are usually used as tool edges or welding electrodes.

A: For tungsten wire, the diameter is from 0.008mm~3.2mm.
For the tungsten rod, the diameter is from 2mm~100mm, length is from 50mm~2000mm.
For the tungsten sheet, the thickness is from 0.025mm~2mm, the width is from 50mm~500mm, and the max length is 1000 mm.
For the tungsten plate, the thickness is from 2.1~25mm, the width is from 30mm~600mm, and the max length is 1000mm.
For a tungsten boat, the thickness is from 0.2mm~0.5mm, the width is from 5mm~25mm, and the max length is 1000mm.
For the tungsten tube, the diameter is from 25mm~340mm, and the max length is 650mm.
For the tungsten crucible, the diameter is from 10mm~500mm, the height is from 10mm~750mm, and the thickness is from 2mm~20mm.
Q: what is the surface of your tungsten products?
A: For tungsten wire, we have a graphite black surface, an alkali cleaning surface, and an electric polished surface.
For tungsten rod&sheet&plate&boat&tube&crucible,etc
We have a black surface, an alkali-cleaning white surface, bright surface (machine, polished, ground).
Other Tungsten related products