Stamped titanium mesh is a material commonly used in filtration, screening, and other applications, and is usually made of pure titanium. Below are some common stamped titanium mesh specifications. Actual specifications may vary depending on the specific application and manufacturer.
- Material: Pure titanium, such as CP1 (one of the common pure titanium).
- Thickness: Typically between 0.5 mm and 2 mm, depending on application requirements.
- Mesh hole size: Pore size can vary depending on the requirements of filtration or screening. Common aperture sizes range from 3.5x4 to 14x40 mm.
- Hole Pitch: Hole pitch refers to the distance between the centers of adjacent holes. It also depends on the specific application needs and can be customized according to customer requirements.
- Surface Treatment: Some stamped titanium mesh screens may require surface treatment, such as pickling or plating, to meet specific performance requirements.
- Dimensions: Length and width dimensions will vary depending on specific usage scenarios and customer needs. Some applications may require large stamped titanium mesh, while other applications may require smaller sizes.
- Shape: Stamped titanium mesh can be made into different shapes according to needs, such as square, rectangular, round, etc.
Size and allowable tolerance of the titanium mesh sheet.
| Thickness/mm | Thick tolerance | Mesh wide | Wide tolerance | Mesh length | Length tolerance |
| >0.5 | ±0.05 | 400~1200 | +15/0 | <=2000 | +20/0 |
| >0.5~0.8 | ±0.07 | ||||
| >0.8~1.1 | ±0.09 | ||||
| >1.1~1.5 | ±0.11 |

| LWM(B) | Tolerance | SWD(A) | Tolerance | Cut stem(F) | Tolerance |
| 4 | ±0.1 | 3.5 | ±0.2 | 0.5 | ±0.2 |
| 6.1 | ±0.15 | 3.7 | ±0.2 | 0.8 | ±0.1 |
| 8 | ±0.15 | 4.5 | ±0.2 | 1.5 | ±0.1 |
| 10 | ±0.15 | 4.5 | ±0.2 | 1.5 | ±0.15 |
| 10 | ±0.15 | 5 | ±0.2 | 1.52 | ±0.15 |
| 10.3 | ±0.15 | 6 | ±0.2 | 1.5 | ±0.15 |
| 12.5 | ±0.15 | 4.5~6.5 | ±0.2 | 1.7 | ±0.2 |
| 12.5 | ±0.15 | 5.6 | ±0.2 | 1.8 | ±0.2 |
| 13 | ±0.15 | 5.5 | ±0.2 | 1.5 | ±0.2 |
| 13 | ±0.15 | 5.8 | ±0.2 | 1.9 | ±0.2 |
| 20 | ±0.20 | 7 | ±0.2 | 1.7 | ±0.2 |
| 40 | ±0.20 | 14 | ±0.2 | 1.7 | ±0.2 |

How much does titanium mesh cost?
The cost of titanium mesh can vary based on several factors, including the grade of titanium, the thickness and dimensions of the mesh, and the supplier. Titanium is generally an expensive material, and its cost can fluctuate based on market conditions and availability.