Electrochemical Water Treatment - Titanium Anode Application

May 17, 2023

The basic principle of electrochemical water treatment titanium anode technology is to cause pollutants to undergo direct electrochemical reaction or indirect electrochemical conversion on the electrode, namely direct electrolysis and indirect electrolysis.

Direct electrolysis refers to the removal of pollutants from wastewater by direct oxidation or reduction at the electrode. Direct electrolysis can be divided into an anode process and a cathode process; Indirect electrolysis refers to the use of redox substances generated by electrochemistry as reactants or catalysts to convert pollutants into less toxic substances. Indirect electrolysis can be divided into reversible processes and nonreversible processes.

1、 Classification of Electrochemical Water Treatment Technologies

1. Electrocoagulation electric flotation method: Under the action of external voltage, the anode is oxidized to produce a large number of cations, which then form colloids to condense the pollutants in the wastewater. At the same time, a large amount of hydrogen gas is generated on the cathode to form microbubbles and adhere to the flocs for flotation. This method is called electrocoagulation electric flotation.

2. Electrodeposition method: By utilizing the potential difference of different metal components in the electrolyte, soluble metals in the free or bound state are precipitated at the cathode. The appropriate potential is the key to the occurrence of electrodeposition.

3. Electrochemical oxidation method: Electrochemical oxidation is divided into direct oxidation and indirect oxidation, which belong to the anodic reaction process. Direct oxidation refers to the direct conversion of pollutants into harmless substances through anodic oxidation; Indirect oxidation refers to the production of intermediate substances with strong oxidizing effects through anodic reactions or the occurrence of intermediate reactions beyond anodic reactions, resulting in the oxidation of the treated pollutants and their eventual conversion into harmless substances.

4. Electrodialysis method: depending on the unique function of selectively penetrating the membrane under the action of the electric field, ions can enter from one solution into another to achieve the separation and concentration of ionized pollutants. When electrodialysis water is used to treat titanium anode metal ions, solid metal can not be recovered directly, but the concentrated salt solution can be obtained, and the effluent quality can be significantly improved.

5. Electrochemical membrane separation method: A separation process that utilizes the potential difference on both sides of the membrane, commonly used for the separation of gaseous pollutants.

3、 Advantages of Electrochemical Water Treatment Technology

1. The hydroxyl radicals generated during the electrolysis process of titanium electrodes can directly react with organic pollutants in wastewater, degrading them into carbon dioxide, water, and simple organic compounds, without or with little secondary pollution. It is an environmental high-tech.

2. DSA can save energy (>23%) in the chlor alkali industry with high energy efficiency. The electrochemical process can be carried out at normal temperature and pressure.

3. Electrochemical methods can be used alone or in combination with other treatment methods, such as as as pre-treatment methods, to improve the biodegradability of wastewater.

4. Electrolytic equipment and its operation are generally relatively simple and cost-effective.