We adhere to the corporate values of "environmental protection, trustworthiness, efficiency and pragmatism", and strive to make ourselves a first-class enterprise in this Titanium Material, ASTM B348 Grade 12 Titanium Bar, 6-6-2 titanium industry. We continue to optimize the process parameters, our products meet the needs of market diversification. Our innovative R&D system is gradually improved, the innovation mechanism is gradually improved, and the comprehensive strength is continuously enhanced.

1. Product Introduction

Gr1 titanium bar is a solid bar made of 99.5% titanium with a silver-white bright surface. It is made of pure titanium Grade 1, often used in aerospace, medical and chemical applications. These bars possess a low density, high strength, excellent corrosion resistance, and good weldability. 

2. Basic Information

Titanium bar Shape: Round, Square, and Rectangular

Dimensions: Custom-made size available

Titanium rod production status:

Hot processing state (R)

Cold working state (Y)

Annealing state (M)

3. Gr1 titanium bar chemical and mechanical properties according to ASTMB348

chemical elements N C H Fe O Residuals max each Residuals max total
Grade1 0.03 0.08 0.015 0.2 0.18 0.1 0.4
Grade tensile strength Mpa yield strength Mpa elongation
Grade1 240 138 24

4. Titanium rod application:

Gr1 titanium bars can be used in environments up to 400°C and offer good resistance to general corrosion, pitting, and crevice corrosion. They can be easily machined, forged, or welded using common titanium fabrication techniques. These bars are available in various sizes and lengths, making them suitable for various applications, including bolts, fasteners, rivets, bicycle frames, and more.

We provide titanium rods for various industries. The most common applications of this material include aviation, the petrochemical industry, the construction of water treatment plants, power generation facilities, and offshore vehicles.

Detail Shows

titanium rod
6mm titanium rod

5. Permissible tolerance for Titanium Bars-Hot-Rolled Round and Square bars

Specified Size, in. (mm) Size Variations,
in. (mm)
Out-of-Round A or Out-of-Square, B in. (mm)
1 ⁄ 4 to 5 ⁄ 16 (6.35 to 7.94), incl ±0.005 (0.13) 0.008 (0.20)
5 ⁄ 16 to 7 ⁄ 16 (7.94 to 11.11), incl ±0.006 (0.15) 0.009 (0.23)
7 ⁄ 16 to 5 ⁄ 8 (11.11 to 15.88), incl ±0.007 (0.18) 0.010 (0.25)
5 ⁄ 8 to 7 ⁄ 8 (15.88 to 22.22), incl ±.008 (0.20) 0.012 (0.30)
7 ⁄ 8 to 1 (22.22 to 25.40), incl ±0.009 (0.23) 0.013 (0.33)
Over 1 to 1 1 ⁄ 8 (25.40 to 28.58), incl ±0.010 (0.25) 0.015 (0.38)
Over 1 1 ⁄ 8 to 1 1 ⁄ 4 (28.58 to 31.75), incl ±0.011 (0.28) 0.016 (0.41)
Over 1 1 ⁄ 4 to 1 3 ⁄ 8 (31.75 to 34.92), incl ±0.012 (0.30) 0.018 (0.46)
Over 1 3 ⁄ 8 to 1 1 ⁄ 2 (34.92 to 38.10), incl ±0.014 (0.36) 0.021 (0.53)
Over 1 1 ⁄ 2 to 2 (38.10 to 50.80), incl ± 6 1 ⁄ 64 (0.40) 0.023 (0.58)
Over 2 to 2 1 ⁄ 2 (50.80 to 63.50), incl + 1 ⁄ 32 , − 0 (0.79) 0.023 (0.58)
Over 2 1 ⁄ 2 to 3 1 ⁄ 2 (63.50 to 88.90), incl + 3 ⁄ 64 , − 0 (1.19) 0.035 (0.89)
Over 3 1 ⁄ 2 to 4 1 ⁄ 2 (88.90 to 114.30), incl + 1 ⁄ 16 , − 0 (1.59) 0.046 (1.17)
FAQ

Q: 1. What grades of pure titanium bars are there?

A: Common grades of pure titanium bars include: Gr1, Gr2, Gr3, Gr4, etc. Among them, the Gr1 titanium bar is the softest and has the highest purity, and so on.

Q: 2. What are the implementation standards of pure titanium bars?

A: The common implementation standards of Gr1 titanium bar and Gr2~Gr4 titanium bar are ASTMB348, ASTMF67, etc. German standards, Russian standards, and French standards can be customized according to requirements.

Q: 3. What is the purity of the Gr1 titanium bar?

A: The purity of the Gr1 titanium bar can reach more than 99.7%, and higher purity can be customized according to requirements.

Q: 4. Is the Gr1 titanium bar in stock?

A: Some specifications of the Gr1 titanium bar are in stock, and all specifications of the Gr2 and Gr5 titanium bars are in stock.

Q: 5. Can the Gr1 titanium bar be cut in half?

A: Gr1 titanium bar can be cut to length according to customer requirements, and can be sent by express, air, or sea.

Contact information:

Tel: +86-0917- 3664600

Whatsapp: +8618791798690

Email: sales@tmsalloy.com
tina@tmsalloy.com

With advanced consciousness, brand-new concepts and innovative spirits, we integrate advanced technologies at home and abroad to continuously research and develop new Top Quality 99.99% Pure Titanium Rod Bars of Price Per Kg for the industry. We enhance the overall quality of the enterprise, strengthen the core competitiveness of the enterprise, and lay a solid foundation for the realization of the enterprise development strategy. Employees bring more vigor and vitality to the company, and their active and enthusiastic participation will enable the company to continue to progress and develop and grow.

Hot Tags: High Purity ASTMB348 Gr1 Titanium Bar, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, buying nickel bars, Titanium Plating Baskets, Grade 5 Titanium Spring, Welded Titanium Tubing, titanium hiking stove, 1 titanium tubing

You May Also Like
Send Inquiry