Titanium Alloy Fal-Zinc Alloy Sheet

Titanium Alloy Fal-Zinc Alloy Sheet

Ti0.3mo0.8ni titanium sheet
UNS R53400
Send Inquiry
Chat Now
Description

For us, providing better buy nickel stub end, tantalum plate hs code, titanium alloy tube in terms of quality and design is our only way out in the market competition. The company guides technological innovation to lead the development of the industry, integrity management promotes social progress, the courage to assume social responsibilities, and dedication to love. According to the individual needs of the employees, we formulate the behavior norms and assessment measures appropriately to optimize the allocation of human resources.

Products Introduction

1. Optimal ASMA code design, enhanced strength, superior crevice corrosion resistance, and exceptional resistance under oxidizing to moderately reducing conditions, particularly chlorides, are all features of Gr12 titanium plate, a close relative of alpha titanium.

2. Basic Information

product nameGr12 Titanium platethickness0.3-60MM
product materialGr12 Ti0.3Mo0.8NiWidth1000/1200/1220/1500/2000
applicationsIndustrialLengthCan be cut and customized
Supply statusHot-working, cold-working, annealing, solid solutionSupply standardASTMB265

Gr12 Chemical composition:

Grade

N

C

H

Fe

O

Al

V

Pa

Mo

Ni

Ti

Gr12

0.03

0.08

0.015

0.30

0.25

/

/

/

0.2~0.4

0.6~0.9

bal

Ti0.3Mo0.8Ni Tensile properties:

Grade

Tensile strength(min)

Yield strength(min)Elongation (%)

Ksi

MPa

Ksi

MPa


12

70

438

50

345

18

Detail Shows


Gr12 titanium plate

Gr12 titanium plate

ti0.3mo0.8ni titanium sheet

Ti0.3mo0.8ni titanium sheet

3. The nominal composition of the Gr12 titanium sheet

Titanium molybdenum nickel alloy is Ti-0.3Mo-0.8Ni, which is a Ti-12 alloy researched and developed by the United States in the mid-1970s. It is a titanium alloy resistant to crevice corrosion. The tensile strength of 300 is twice that of pure titanium, the corrosion resistance of reducing media is obviously improved, and crevice corrosion does not occur in the chloride of 150-200.

4. The method used to make Gr12 titanium plate 

The final titanium plate made from the titanium molybdenum nickel alloy ingot, which has undergone forging, rolling, and surface treatment with oxide scale, serves as the raw material for Gr12 titanium plates. The titanium content is about 98.7%, 1% molybdenum nickel alloy (0.3% Mo, 0.8% Ni), and the rest are Fe, O, N, H, and other impurity elements. The cost-production process is similar to that of pure titanium, but the mechanical properties and corrosion resistance are better than pure titanium.

5. Application of Ti0.3mo0.8ni Gr12 titanium plate

(Ti-0.3Mo-0.8Ni) Gr12 titanium plate has good crevice corrosion performance to high temperature, low pH chloride, or weak reducing acid, and its corrosion resistance is significantly better than pure titanium and close to Gr7 alloy.

6. Our advantages

Each department is accountable for the total situation and insists on external training, internal training, and the blending of theory and practice. We are a professional titanium plate supplier and offer Gr12 titanium plates.

gr12 titanium plate supplier tmsalloy.com

Other related titanium sheets 

The most common grades of titanium sheet are Grade 1, Grade 2, Grade 5 (Ti-6Al-4V), and Grade 7. These grades are often used for their high strength-to-weight ratio, corrosion resistance, and biocompatibility. Other grades that are also used, but less commonly, include Grade 9 (Ti-3Al-2.5V) and Grade 12 (Ti-0.3Mo-0.8Ni). The choice of grade depends on the specific application requirements, such as temperature resistance, strength, and chemical resistance.

gr5 titanium plate cost

With our unremitting pursuit of Titanium Alloy Fal-Zinc Alloy Sheet details and perfection, we have been widely praised by customers and won wide trust from all walks of life. We have become one of the most trustworthy brands of industry users. We strive to achieve greater breakthroughs in performance, and strongly promote project operations and focus on building the company's image project. We build our brand with rigorous and meticulous spirit and serve customers with a warm and thoughtful attitude.

Hot Tags: ASME SB265 UNS R53400 DIN 3.7105 Gr12 Titanium Plate, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Zirconium Wires, molybdenum wire mesh, short stub end, Ruthenium Iridium Titanium Anode, Gr5 Titanium Alloy Bar, Zirconium Crucible