Tc4 Titanium Alloy Bar

Tc4 Titanium Alloy Bar

Gr5 titanium bar
UNS R56400
BT6 DIN3.7165
Send Inquiry
Chat Now
Description

With the development theme of innovation, hard work and integrity, we are striving to become a well-known enterprise of Titanium Washer, Titanium Material, Nickel 200 Wire. We carry out our corporate social responsibility management purpose and innovate lifestyles to contribute to society and the future. Our goal is to provide the products with best value and highest quality and sales support to our valued customers all over the world. We sincerely welcome you to visit our factory and looking forward to a long-term cooperation with you. It is the strong support from all walks of life that our company has been able to speed up its development, grow its development scale and improve its development quality.

Products Introduction

1. Aluminum and vanadium are added to the titanium alloy used to make 6al4v Titanium Rod. This material has very high corrosion resistance. It typically has a density of 4.51g/cm3, which is only 60% of steel.

2. Basic Information

Titanium bar ASTMB348 products in various sizes, shapes, and types.

Shape: round, flat, rectangle, square, etc.

Sizes for GR5 titanium rods include 5mm to 100mm in diameter, 100mm to 3000mm in length, and customizable lengths.

Detail Shows

timascus round bar

Gr5 titanium bar

Grade 5 Round Bar

Grade 5 Round Bar ASTMB348

3. What are the properties and chemical makeup of the 6al4v titanium rod?

Ti-6Al-4V and Ti 6-4 rods are other names for 6al4v titanium rods. ti-6al-4v-Eli should not be confused with it (grade 23). It is the most commonly used alloy. Its chemical composition consists of residual titanium, 6% aluminum, 4% vanadium, 0.25% (maximum) iron, and 0.2% (maximum) oxygen. Its strength is comparable to that of commercially pure titanium (grades 1-4), and it shares the same stiffness and thermal characteristics with grade 5 (except thermal conductivity, which is approximately 60% lower). Heat treatability is one of its numerous benefits. The qualities of strength, corrosion resistance, weldability, and manufacturability are all present in this grade in the ideal proportions.

1 kilo titanium bar

Titanium bar

titanium alloy bar

Titanium alloy bar

 

4. 6al4v titanium rod applications

Stronger than many steel alloy structural bars are several high-strength titanium alloys. Therefore, compared to other metal structural materials, 6al4v titanium rods have substantially greater specific strength (strength/density) and can be used to create pieces with high strength units, good stiffness, and lightweight. The grade of titanium alloy with the greatest utility is this one. It is commonly utilized for shafts, bolts, screws, and other components of structures.

6al4v titanium rod for sale

5. Why choose us?

As a high-quality 6al4v titanium rod manufacturer, we also have some similar grades of Gr5 6al4v, such as:

Ti-6Al-4V, Ti-6Al-4V ELI, Ti-6Al-4V SP, Ti-6Al-4V ELI SP (USA)

BT-6, BT-6C, BT-6К, BT-6КТ (Russia);

IMI-318, IMI-318ELI (UK);

TiAl6V4 (Germany); T-A6V (France); SAT-64 (Japan).

To contact us and purchase titanium rods right away, go to sales@tmsalloy.com.

FAQ

Q: 1. What is the composition of the 6al4v Titanium Rod?

A: According to ASTMB348 standard, the composition of Ti6AI-4V Titanium Rod is as follows
Aluminum 5.50 to 6.75%
Vanadium 3.50 to 4.50%
Oxygen (max) 0.020%
Iron (max) 0.40%
Carbon (max) 0.10%
Nitrogen 0.05%
Hydrogen (max) 0.015%
Others, total (max) 0.40%
*Others, each (max) = 0.1%
Titanium Others

Q: 2. What is the price of TA6V 6al4v Titanium material?

A: The price of the TA6V 6al4v Titanium Rod varies according to the outer diameter, and the price varies according to the fixed length or random length, specifically ranging from 120~230RMB/KG.

Contact information:

Tel: +86-0917- 3664600

Whatsapp: +8618791798690

Email: sales@tmsalloy.com
tina@tmsalloy.com

Our company has established its own independent research and development team, constantly develop new Tc4 Titanium Alloy Bar and improve old products. We attach great importance to customer service, especially the establishment of a technical support department and after-sales service department. We are further enhancing the technical level of our employees and injecting high technology into our products to provide better and more affordable products to our customers abroad.

Hot Tags: UNS R56400 TA6V ASTMB348 Gr5 6al4v Titanium Rod, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Molybdenum Bar, Gr5 Titanium Plate, Titanium Nuts, Zirconium Crucible, Molybdenum Boat, Ruthenium Iridium Titanium Anode

You May Also Like
Send Inquiry