Description

We will combine our practical experience to design the titanium welding rod, Titanium Grade 5 Ti 6Al 4V Rods, CP2 TI GR 2 Seamless Tubing equipment that meets various process requirements. Our company has developed the market through various measures and channels, especially the international market. We are committed to providing our customers with safe and innovative products, services and solutions to achieve profitable growth. We shoulder the responsibility of leading the development of the industry, follow the pace of the great rejuvenation of the Chinese nation, and go to the world. The society is based on our trust, and we return the warmth to the society.

Products Introduction

1. Grade 2 Titanium Wires are made of commercially pure titanium, which is a silver-white metal, it has many excellent properties, such as being ultra-corrosion-resistant.

2. Basic Information

Temper rating: Softened (Annealed)

Grade: GR1, GR2, GR3, Gr4, Ti6AL7Nb, Ti13Nb13Zr, Ti1533

The main standard of titanium wire: AMS4956, JIS, ASTM B863 AWSA5.16

Detail Shows

Gr2 titanium wire price
Gr2 Titanium wire

3. The applications of Gr2 Titanium Wires

Gr2 Titanium wires products are widely used in the section aerospace, aviation, navigation, military industry, power engineering, environmental protection equipment, construction industry, and daily necessities.

Due to its excellent corrosion resistance, Gr2 titanium wire has been widely applied in chemical, pharmaceutical, papermaking, and other industries because of its excellent corrosion resistance. It can be woven into a net to be used as a seawater filter, a pure water filter, and a chemical filter.

4. Pure titanium wires mechanical properties acc to ASTMB863

Gradetensile yieldStandards
Gr1240ASTMB863
Gr2345ASTMB863
Gr3450ASTMB863
Gr4550ASTMB863

Gr2 Titanium wires supplier
Gr2 titanium wire manufactures

5. What are the other types of titanium wires except for grade 2 titanium wires?

According to the application and material, titanium wire can be divided into pure titanium eyeglass wire, titanium straight wire, pure titanium wire, titanium welding wire, titanium hanger wire, and bright titanium wire, titanium medical wire, nickel-titanium wire.

Gr2 titanium wires for sale

6. Our advantages:

After years of development, we have full series of titanium wire products, such as ERTi2, ERTi7, ERTi12, and ERTi23 wires. Gr2, and Gr12 titanium wire stock, metal marking is also available, and other custom sizes also can be ordered and with fast delivery.

Reasonable price

Short and fast delivery

The MOQ is small 5~10kg

Logistics use FEDEX DHL mainstream express, delivery safety, and guaranteed.

Support third-party inspection

Send inquiry to us for quotations at sales@tmsalloy.com

We take Oxford Alloy Ti-7/Pure Ti Wire/Erti-7 for Welding that cater to and meet the needs of customers as our responsibility, and we have an independent research and development department to continuously introduce new ones. We unite all employees to provide high-quality products and services to the society and achieve common prosperity in the industry. We've established long-term, stable and good business relationships with many manufacturers and wholesalers around the world.

Hot Tags: gr2 titanium wires, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, titanium filler wires, Titanium Gr 7 BAR, titanium v band flange, Titanium grade 2 Bolt, Titanium Grade 4 Bar rod, Titanium Grade 1 Sheet

You May Also Like
Send Inquiry