Relying on the advantages of technology research and development in the field of Titanium Grade 2 Welded Pipe, Torispherical Dished Head Supplier, metal zirconium crucible and rich production experience, we can provide customers with one-stop comprehensive solutions such as product design and development, testing, mass production, and follow-up tracking services. We use the development thought to adjust production and innovate by means of reform. Creating a diversified team has gradually become an inevitable trend for our company to participate in international competition.
1. Product Introduction
Gr1 titanium bar is a solid bar made of 99.5% titanium with a silver-white bright surface. It is made of pure titanium Grade 1, often used in aerospace, medical and chemical applications. These bars possess a low density, high strength, excellent corrosion resistance, and good weldability.
2. Basic Information
Titanium bar Shape: Round, Square, and Rectangular
Dimensions: Custom-made size available
Titanium rod production status:
Hot processing state (R)
Cold working state (Y)
Annealing state (M)
3. Gr1 titanium bar chemical and mechanical properties according to ASTMB348
chemical elements | N | C | H | Fe | O | Residuals max each | Residuals max total |
Grade1 | 0.03 | 0.08 | 0.015 | 0.2 | 0.18 | 0.1 | 0.4 |
Grade | tensile strength Mpa | yield strength Mpa | elongation |
Grade1 | 240 | 138 | 24 |
4. Titanium rod application:
Gr1 titanium bars can be used in environments up to 400°C and offer good resistance to general corrosion, pitting, and crevice corrosion. They can be easily machined, forged, or welded using common titanium fabrication techniques. These bars are available in various sizes and lengths, making them suitable for various applications, including bolts, fasteners, rivets, bicycle frames, and more.
We provide titanium rods for various industries. The most common applications of this material include aviation, the petrochemical industry, the construction of water treatment plants, power generation facilities, and offshore vehicles.
Detail Shows


5. Permissible tolerance for Titanium Bars-Hot-Rolled Round and Square bars
Specified Size, in. (mm) | Size Variations, in. (mm) |
Out-of-Round A or Out-of-Square, B in. (mm) |
1 ⁄ 4 to 5 ⁄ 16 (6.35 to 7.94), incl | ±0.005 (0.13) | 0.008 (0.20) |
5 ⁄ 16 to 7 ⁄ 16 (7.94 to 11.11), incl | ±0.006 (0.15) | 0.009 (0.23) |
7 ⁄ 16 to 5 ⁄ 8 (11.11 to 15.88), incl | ±0.007 (0.18) | 0.010 (0.25) |
5 ⁄ 8 to 7 ⁄ 8 (15.88 to 22.22), incl | ±.008 (0.20) | 0.012 (0.30) |
7 ⁄ 8 to 1 (22.22 to 25.40), incl | ±0.009 (0.23) | 0.013 (0.33) |
Over 1 to 1 1 ⁄ 8 (25.40 to 28.58), incl | ±0.010 (0.25) | 0.015 (0.38) |
Over 1 1 ⁄ 8 to 1 1 ⁄ 4 (28.58 to 31.75), incl | ±0.011 (0.28) | 0.016 (0.41) |
Over 1 1 ⁄ 4 to 1 3 ⁄ 8 (31.75 to 34.92), incl | ±0.012 (0.30) | 0.018 (0.46) |
Over 1 3 ⁄ 8 to 1 1 ⁄ 2 (34.92 to 38.10), incl | ±0.014 (0.36) | 0.021 (0.53) |
Over 1 1 ⁄ 2 to 2 (38.10 to 50.80), incl | ± 6 1 ⁄ 64 (0.40) | 0.023 (0.58) |
Over 2 to 2 1 ⁄ 2 (50.80 to 63.50), incl | + 1 ⁄ 32 , − 0 (0.79) | 0.023 (0.58) |
Over 2 1 ⁄ 2 to 3 1 ⁄ 2 (63.50 to 88.90), incl | + 3 ⁄ 64 , − 0 (1.19) | 0.035 (0.89) |
Over 3 1 ⁄ 2 to 4 1 ⁄ 2 (88.90 to 114.30), incl | + 1 ⁄ 16 , − 0 (1.59) | 0.046 (1.17) |
FAQ
Q: 1. What grades of pure titanium bars are there?
Q: 2. What are the implementation standards of pure titanium bars?
Q: 3. What is the purity of the Gr1 titanium bar?
Q: 4. Is the Gr1 titanium bar in stock?
Q: 5. Can the Gr1 titanium bar be cut in half?
Contact information:
Tel: +86-0917- 3664600
Whatsapp: +8618791798690
Email: sales@tmsalloy.com
tina@tmsalloy.com
With strict quality management and dedicated work attitude, we are sure to bring satisfactory M12× 25 Zinc Plated Titanium Full Threaded Rod to our customers. Our company comprehensive strength has been rapidly improved, the market share of products has steadily increased, with excellent quality, high-quality services, won the broad praise of the majority of consumers. We wholeheartedly welcome the patronage of new and old customers from all walks of life, and work with you towards a better, stronger and higher goal!
Hot Tags: High Purity ASTMB348 Gr1 Titanium Bar, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, titanium strip coil, titanium tube sheet for exchanger, Titanium bellows expansion joints, Tungsten Bar, titanium m6 allen bolts, nickel 200 pipe