Our company adheres to the tenet of 'Because of focus, so professional!' After long-term unremitting efforts, our company has developed into a modern perforated titanium sheet, polished titanium sheet, TUNGSTEN crucible for melting steel manufacturing enterprise with strong core competitiveness. Our company has a sound production management system, strong technical force, and has independent intellectual property rights, is your best choice for cooperation. To meet the needs of customers with advanced technology, mature products and perfect service is the main purpose of our company. Our factory management has been institutionalized, standardized and scientific. Our company is committed to building a stable and enthusiastic working team, emphasizing in-depth and close communication and cooperation with customers and partners.
Products Introduction
1. Zirconium crucible is used to contain reaction chemicals in the laboratory environment, so it must be able to withstand high temperatures and a variety of acids.
2. Basic information
Zirconium 702 crucible Size: 20 25 35 45 55 75 100 500 1000ml
3. The properties of Zirconium crucible
The density of the zirconium is 6.51g/com3, the purity is 99.6%, and the maximum service temperature is 2200 ℃. It is mainly used for smelting rare and precious metals, with good thermal stability.
Detail Show

zirconium crucible price

zirconium 702 crucible
4. Advantages of zirconium crucible
Compare with other crucible types, such as steel, platinum, porcelain, glass, or nickel. Although more expensive than glass, steel, or nickel, the advantages provided by these zirconium crucibles make it more cost-effective and it is significantly less expensive than platinum and other noble metals, with other material advantages.
These advantages include the high oxidation resistance of the zirconium crucible.
Highly resistant to most acids and alkalis.
Completely solvent resistant (except hydrofluoric acid).
The zirconium crucible will not form an alloy with metal.
Can almost eliminate sample contamination
5. Packing and delivery
Packed in wooden boxes with plastic partitions, the weight of a single box does not exceed 100kg.
Delivery with DHL, FedEx, TNT, etc by express delivery or by sea and by air from the main port of China.
6. Our advantages
Professional corrosion-resistant metal suppliers, zirconium crucible suppliers, and zirconium crucible can be customized according to customer requirements. In addition, with the optimization of the company's marketing network, it has a nationwide sales network and a complete after-sales service system, forming a marketing network system with rapid response, efficient coordination, and all-around services.
Looking to the future, we keep up with the emerging application fields and keep our High Temperature Large Alumina Ceramic Crucible for Melting Metal and services in line with the development trend of the times. Our company in the continuous development of market share at the same time, pay more attention to the improvement of our overall strength. We strive to meet and even surpass our customers' needs, and become long-term, win-win partners with our customers.
Hot Tags: zirconium crucible, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Ti Strip ASTMF67, Gr2 Titanium Sheet, Ruthenium Iridium Titanium Anode, Titanium Slotted Flat Head Screws, Titanium Alloy Valve, Square Structural Tubing titanium