We promise to provide our customers with stable product quality of the molybdenum bar stock, Gr2 Titanium Welding Wires, Titanium Grade 4 Sheets Plates Coils, good business reputation and perfect after-sales service. We have rich production experience and our products are widely used in different fields. We use a strong faith and perseverance to establish the company's product reputation and corporate image.
1. Product Introduction
Gr1 titanium bar is a solid bar made of 99.5% titanium with a silver-white bright surface. It is made of pure titanium Grade 1, often used in aerospace, medical and chemical applications. These bars possess a low density, high strength, excellent corrosion resistance, and good weldability.
2. Basic Information
Titanium bar Shape: Round, Square, and Rectangular
Dimensions: Custom-made size available
Titanium rod production status:
Hot processing state (R)
Cold working state (Y)
Annealing state (M)
3. Gr1 titanium bar chemical and mechanical properties according to ASTMB348
chemical elements | N | C | H | Fe | O | Residuals max each | Residuals max total |
Grade1 | 0.03 | 0.08 | 0.015 | 0.2 | 0.18 | 0.1 | 0.4 |
Grade | tensile strength Mpa | yield strength Mpa | elongation |
Grade1 | 240 | 138 | 24 |
4. Titanium rod application:
Gr1 titanium bars can be used in environments up to 400°C and offer good resistance to general corrosion, pitting, and crevice corrosion. They can be easily machined, forged, or welded using common titanium fabrication techniques. These bars are available in various sizes and lengths, making them suitable for various applications, including bolts, fasteners, rivets, bicycle frames, and more.
We provide titanium rods for various industries. The most common applications of this material include aviation, the petrochemical industry, the construction of water treatment plants, power generation facilities, and offshore vehicles.
Detail Shows


5. Permissible tolerance for Titanium Bars-Hot-Rolled Round and Square bars
Specified Size, in. (mm) | Size Variations, in. (mm) |
Out-of-Round A or Out-of-Square, B in. (mm) |
1 ⁄ 4 to 5 ⁄ 16 (6.35 to 7.94), incl | ±0.005 (0.13) | 0.008 (0.20) |
5 ⁄ 16 to 7 ⁄ 16 (7.94 to 11.11), incl | ±0.006 (0.15) | 0.009 (0.23) |
7 ⁄ 16 to 5 ⁄ 8 (11.11 to 15.88), incl | ±0.007 (0.18) | 0.010 (0.25) |
5 ⁄ 8 to 7 ⁄ 8 (15.88 to 22.22), incl | ±.008 (0.20) | 0.012 (0.30) |
7 ⁄ 8 to 1 (22.22 to 25.40), incl | ±0.009 (0.23) | 0.013 (0.33) |
Over 1 to 1 1 ⁄ 8 (25.40 to 28.58), incl | ±0.010 (0.25) | 0.015 (0.38) |
Over 1 1 ⁄ 8 to 1 1 ⁄ 4 (28.58 to 31.75), incl | ±0.011 (0.28) | 0.016 (0.41) |
Over 1 1 ⁄ 4 to 1 3 ⁄ 8 (31.75 to 34.92), incl | ±0.012 (0.30) | 0.018 (0.46) |
Over 1 3 ⁄ 8 to 1 1 ⁄ 2 (34.92 to 38.10), incl | ±0.014 (0.36) | 0.021 (0.53) |
Over 1 1 ⁄ 2 to 2 (38.10 to 50.80), incl | ± 6 1 ⁄ 64 (0.40) | 0.023 (0.58) |
Over 2 to 2 1 ⁄ 2 (50.80 to 63.50), incl | + 1 ⁄ 32 , − 0 (0.79) | 0.023 (0.58) |
Over 2 1 ⁄ 2 to 3 1 ⁄ 2 (63.50 to 88.90), incl | + 3 ⁄ 64 , − 0 (1.19) | 0.035 (0.89) |
Over 3 1 ⁄ 2 to 4 1 ⁄ 2 (88.90 to 114.30), incl | + 1 ⁄ 16 , − 0 (1.59) | 0.046 (1.17) |
FAQ
Q: 1. What grades of pure titanium bars are there?
Q: 2. What are the implementation standards of pure titanium bars?
Q: 3. What is the purity of the Gr1 titanium bar?
Q: 4. Is the Gr1 titanium bar in stock?
Q: 5. Can the Gr1 titanium bar be cut in half?
Contact information:
Tel: +86-0917- 3664600
Whatsapp: +8618791798690
Email: sales@tmsalloy.com
tina@tmsalloy.com
We take leading technology, excellent quality, and reasonable price as our survival tenet, and pursue 100% customer satisfaction as our goal to provide customers with the most competitive Factory Wholesale Export Standard Titanium Alloy Bar / Rod ASTM B348 Pure Titanium Price Per Gram Gr1 Gr2 with Best Price. The ultimate goal of our business is to pursue customer satisfaction to the greatest extent. We hope to produce positive social influence, maximize the brand value and realize the sustainable and long-term development of the enterprise.
Hot Tags: High Purity ASTMB348 Gr1 Titanium Bar, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, zirconium crucible price, timascus bar, BT1 0 titanium alloy plate, concentric nickel reducer, Pipe Tee Manufacturers, GR7 Titanium Alloy Bar