We always aim to offer first-class service and high-quality titanium foil roll, nickel teflon tape, titanium mesh plate to our customers and the whole society. You can rest assured that our image is due to our professional technical team. Our team is a well-trained team; a team full of team spirit; a continuous innovation and enterprising team; a team dedicated to serving you in the creed of integrity and pragmatism. Over the years, we have received unanimous praise from users for our good product quality, rigorous work team and technical services. We have set up an up and down personnel mechanism to maximize the potential and creativity of every employee.
Products Introduction
1. BT-20 Titanium Plate is a Russia-grade titanium metal plate, which is one of the titanium alloy plates used in aerospace, aircraft, and other industries like casting, blades, and so on.
2. BT20 titanium plate available size and standards
OD: 1.0~200mm or the customer's size
Standards: ΓOCT23755-87 ΓOCT22178-90 DIN17860-1990
3. Properties of BT20 titanium plate
Titanium Alloy Ti-6Al-1.50 MO-1.5V (BT20) has good comprehensive mechanical properties, the main strengthening mechanism is through the addition of elemental Al to stabilize the elements, Mo and V can improve manufacturability and are increasingly used in the aircraft manufacturing industry.
4. What is the chemical composition of the BT-20 Titanium Plate?
Grade | Chemical composition (mass fraction) (%) is not greater than (except for the specified range value) | ||||||||||||||
Ti | Al | Cr | Mo | Sn | Mn | V | Fe | Si | Zr | C | N | H | O | the sum of other elements | |
BT20 | base | 5.5~7.0 | - | 0.5~2.0 | - | - | 0.8~2.5 | 0.25 | 0.15 | 1.5~2.5 | 0.1 | 0.05 | 0.015 | 0.15 | 0.3 |
5. The main properties of high-temperature titanium alloys
Designation | The maxim temperature of usage,℃ |
RT tensile | High temperature tensile | Durability | ||||||||
δb MPa |
δ0.2 MPa |
δ5 % |
Ψ % |
℃ | δb MPa |
δ5 % |
Ψ % |
℃ |
δb Mpa |
T h. |
||
TC4 | 300 | 900 | 830 | 10 | 25 | 400 | 615 | 12 | 40 | 400 | 570 | 100 |
BT20 | 350 | 930 | - | 7-10 | - | 350 | 685 | - | - | 350 | 665 | 50 |
500 | 570 | - | - | 500 | 470 | 50 | ||||||
TA7 | 350 | 785 | 680 | 10 | 25 | 350 | 490 | - | - | 350 | 440 | 100 |
Ti-17 | 370 or 400 | 1120 | 1030 | 7 | 15 | 370 | 907 | 12 | 30 | 370 | 685 | 100 |
Ti-811 | 400 | 895 | 825 | 10 | 20 | 425 | 620 | 10 | 25 | - | - | - |
TC6 | 400 or 450 | 980 | 840 | 10 | 25 | 400 | 735 | - | - | 400 | 665 | 100 |
TC11 | 500 or 530 | 1030 | 900 | 10 | 30 | 500 | 685 | - | - | 500 | 595 | 100 |
Ti-6242s | 520 | 895 | 825 | 10 | 25 | 480 | 620 | 10 | 25 | 525 | 480 | 35 |
Ti-55 | 550 | 980 | 900 | 10 | 25 | 550 | 610 | 12 | 30 | 550 | 430 | 100 |
Ti-60 | 600 | 1100 | 1030 | 11 | 18 | 600 | 700 | 14 | 27 | 600 | 350 | 100 |
6. How is the application of the BT-20 Titanium Plate?
BT20 alloy is mainly used for manufacturing structural parts and welding load-bearing parts with continuous working hours under temperatures below 500℃.
Its products are used in a variety of engine blades, casing, aircraft, and other stamping parts.
7. Our advantages
To achieve our development vision, we provide our customers with high-quality products and good after-sales service. Titanium alloy BT20 titanium plate won the majority of crucial certifications in its market. We are one of the superior Titanium Alloy Ti-6Al-1.50 MO-1.5V (BT20) plates suppliers, we have sales offices in different cities of domestic. Our head office is located in Baoji and we supply Titanium Alloy Ti-6Al-1.50 MO-1.5V (BT20) sheets and plates to all major cities of China from Baoji.
FAQ
Q: 1. What is the corresponding grade of BT20 titanium alloy?
Q: 2. What are the mechanical properties of BT20 titanium alloy?
Q: 3. What is the annealing temperature of the BT20 titanium plate?
Q: 4. What fields are BT20 titanium alloy mainly used in?
Contact information:
Tel: +86-0917- 3664600
Whatsapp: +8618791798690
Email: sales@tmsalloy.com
tina@tmsalloy.com
We will continue to use leading technology, high-efficiency production organization and quality control capabilities to make us the most competitive and specialized Data Sheet of Avimetal AM TC11(BT9) Powder company. Our company relies on high-tech and high-quality products and perfect services to create good economic and social benefits. We have gradually formed a management team with innovative consciousness, innovative spirit, knowledge of technology and management.
Hot Tags: Aerospace Ti-alloy TA15 B-T20 Titanium Plate, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, TiCu Clad, titanium screws for bikes m5 stem bolts, Titanium screw Slotted Flat Head, TUNGSTEN plate price, titanium flange bolts, Ti0 2Pd alloy plate