Data Sheet of Avimetal AM TA15 (BT20) Powder

Data Sheet of Avimetal AM TA15 (BT20) Powder

Titanium Alloy Sheet (BT20)
China Titanium Alloy Sheet (BT20)
Titanium Alloy Ti-6Al-1.50 MO-1.5V (BT20) Sheets
VT20 BT20 titanium sheet
Send Inquiry
Chat Now
Description

We produce quality zirconium crucible zirconium crucible temperature, titanium fittings, Buy Titanium Welding Rods, creating social wealth and achieving common prosperity. Quality management has become the cornerstone of our economic development and our penetration into the global market. We take the core of the corporate culture of looking into the overall situation, seeking truth and being pragmatic as the connotation, and uphold the spirit of dare to take responsibility and dare to be responsible.

Products Introduction

1. BT-20 Titanium Plate is a Russia-grade titanium metal plate, which is one of the titanium alloy plates used in aerospace, aircraft, and other industries like casting, blades, and so on.

2. BT20 titanium plate available size and standards

OD: 1.0~200mm or the customer's size

Standards: ΓOCT23755-87 ΓOCT22178-90 DIN17860-1990

3. Properties of BT20 titanium plate

Titanium Alloy Ti-6Al-1.50 MO-1.5V (BT20) has good comprehensive mechanical properties, the main strengthening mechanism is through the addition of elemental Al to stabilize the elements, Mo and V can improve manufacturability and are increasingly used in the aircraft manufacturing industry.

VT20 BT20 titanium sheet for sale

Titanium Alloy Sheet (BT20)

4. What is the chemical composition of the BT-20 Titanium Plate?

Grade Chemical composition (mass fraction) (%) is not greater than (except for the specified range value)
Ti Al Cr Mo Sn Mn V Fe Si Zr C N H O the sum of other elements
BT20 base 5.5~7.0 - 0.5~2.0 - - 0.8~2.5 0.25 0.15 1.5~2.5 0.1 0.05 0.015 0.15 0.3

5. The main properties of high-temperature titanium alloys

Designation The maxim
temperature of
usage,℃
RT tensile High temperature tensile Durability
δb
MPa
δ0.2
MPa

δ5

%

Ψ
%
δb
MPa
δ5
%
Ψ
%

δb

Mpa

T
h.
TC4 300 900 830 10 25 400 615 12 40 400 570 100
BT20 350 930 - 7-10 - 350 685 - - 350 665 50
500 570 - - 500 470 50
TA7 350 785 680 10 25 350 490 - - 350 440 100
Ti-17 370 or 400 1120 1030 7 15 370 907 12 30 370 685 100
Ti-811 400 895 825 10 20 425 620 10 25 - - -
TC6 400 or 450 980 840 10 25 400 735 - - 400 665 100
TC11 500 or 530 1030 900 10 30 500 685 - - 500 595 100
Ti-6242s 520 895 825 10 25 480 620 10 25 525 480 35
Ti-55 550 980 900 10 25 550 610 12 30 550 430 100
Ti-60 600 1100 1030 11 18 600 700 14 27 600 350 100

6. How is the application of the BT-20 Titanium Plate?

BT20 alloy is mainly used for manufacturing structural parts and welding load-bearing parts with continuous working hours under temperatures below 500℃.

Its products are used in a variety of engine blades, casing, aircraft, and other stamping parts.

7. Our advantages

To achieve our development vision, we provide our customers with high-quality products and good after-sales service. Titanium alloy BT20 titanium plate won the majority of crucial certifications in its market. We are one of the superior Titanium Alloy Ti-6Al-1.50 MO-1.5V (BT20) plates suppliers, we have sales offices in different cities of domestic. Our head office is located in Baoji and we supply Titanium Alloy Ti-6Al-1.50 MO-1.5V (BT20) sheets and plates to all major cities of China from Baoji.

FAQ

Q: 1. What is the corresponding grade of BT20 titanium alloy?

A: The chemical composition of BT20 titanium alloy is Ti-6.5Al-1Mo-1V-2Zr and the corresponding domestic grade is TA15 titanium alloy, which has a medium room temperature and high-temperature strength, good thermal stability, and welding performance, and the process plasticity is slightly lower than TC4.

Q: 2. What are the mechanical properties of BT20 titanium alloy?

A: BT20 titanium alloy has high strength and low density, good mechanical properties, and good toughness and corrosion resistance. In addition, the process performance of titanium alloy is poor, cutting is difficult, and it is very easy to absorb impurities such as hydrogen, oxygen, nitrogen, and carbon during hot processing; it also has poor wear resistance and a complex production process.

Q: 3. What is the annealing temperature of the BT20 titanium plate?

A: The stress relief annealing temperature of the BT20 titanium alloy plate is 600-650℃, 0.5-8h, air cooling.

Q: 4. What fields are BT20 titanium alloy mainly used in?

A: The working temperature of the BT20 titanium plate can reach 500℃, and can reach 800℃ instantly (no more than 5min). When working at 450℃, the service life can reach 6000h; it is mainly used to manufacture aircraft, engine parts, and welding load-bearing parts that work for a long time below 500℃.

Contact information:

Tel: +86-0917- 3664600

Whatsapp: +8618791798690

Email: sales@tmsalloy.com
tina@tmsalloy.com

Always customer-oriented, and it's our ultimate goal to get not only by far the most reputable, trustable and honest supplier, but also the partner for Data Sheet of Avimetal AM TA15 (BT20) Powder. With all the business philosophy that is for the sake of consumers, we are enthusiastic to provide high-quality products and good services to new and old customers. Welcome to negotiate and cooperate. We're sure your any inquiry or requirement will get prompt attention, high-quality products, preferential prices and cheap freight.

Hot Tags: Aerospace Ti-alloy TA15 B-T20 Titanium Plate, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Titanium Clad Stainless Steel Plate, gr5 titanium, Buy tantalum foil, monel 400 pipe, Titanium Plating Baskets, Titanium Clad Steel Plate For Chimney

You May Also Like
Send Inquiry