Our company takes the value innovation as the guidance and carries on the Titanium Material, titanium bar ASTM F136, pure titanium sheet brand construction research unceasingly. We will wholeheartedly provide customers with all support and guarantees other than non-core business. In order to adapt to our internationalization strategy and the rapid growth of customer base, we continue to improve the quality and efficiency of customer service support. The company adheres to the business philosophy of "technical innovation, pursuit of quality, and service-oriented". With modern management, professional technology, and high-quality service, we are willing to work with you to create a brilliant tomorrow
1. Phillips flat-head titanium screws are suitable for situations where the nail head is not allowed to be exposed, but corresponding conical countersunk holes must be made on the surface of parts with through holes, it is commonly used to connect two connected parts in machinery, electrical appliances, and buildings.
2. Titanium Phillips Screws available in size and standards
Grade: Gr2 Gr5
Metric thread size:
M10 M2 M2.5 M2.6 M3 M3.5 M4 M5 M6 M8
Metric thread pitch:
0.45mm 0.4mm 0.5mm 0.6mm 0.7mm 0.8mm 1.0mm 1.25mm 1.5mm
Length options:
10.2mm 10.7mm 10mm 12.2mm 12.7mm 12mm 14.2mm 14.7mm 14mm 15mm 16.2mm 16mm 18mm 20mm 25mm 30mm 35mm 4.5mm 40mm 45mm 4mm 5.9mm 50mm 5mm 6.2mm 6mm 7.9mm 8.2mm
Surface: Titanium natural color


3. The characteristic of Titanium Phillips Screws
Flathead Phillips drive titanium screw has high-quality characteristics such as insulation, non-magnetic, corrosion resistance, beautiful appearance, and never rust. Its strength, impact resistance, and mechanical properties are far superior to ordinary stainless steel, the application of titanium screws is becoming more and more diversified, the performance is constantly improving, and the application fields are becoming wider and wider.
4. Titanium Flat Head Screws standards
DIN 965-1990 ISO 7046-1-1994 ASME/ANSI B18.6.3-2-2010
5. Phillips flat head titanium screws size according to DIN 965-1990
Mon | M1.6 | M2 | M2.5 | M3 | M3.5 | M4 | M5 | M6 | M8 |
P | 0.35 | 0.4 | 0.45 | 0.5 | 0.6 | 0.7 | 0.8 | 1 | 1.25 |
dk max | 3 | 3.8 | 4.7 | 5.6 | 6.5 | 7.5 | 9.2 | 11 | 14.5 |
dk min | 2.75 | 3.5 | 4.4 | 5.3 | 6.14 | 7.14 | 8.84 | 10.57 | 14.07 |
k max | 0.96 | 1.2 | 1.5 | 1.65 | 1.93 | 2.2 | 2.5 | 3 | 4 |
No. | 0 | 1 | 1 | 1 | 2 | 2 | 2 | 3 | 4 |
M | 1.7 | 2.35 | 2.7 | 2.9 | 3.9 | 4.4 | 4.6 | 6.6 | 8.7 |
t max | 0.91 | 1.25 | 1.55 | 1.8 | 1.9 | 2.4 | 2.6 | 3.3 | 4.4 |
t min | 0.66 | 0.95 | 1.25 | 1.5 | 1.4 | 1.9 | 2.1 | 2.8 | 3.9 |
6. What is the manufacturing process of Phillips flat-head titanium screws?
Prepare the raw material bar first, and then heated it to 600‑700°C and upset it in a mold to form the shank, head, and R-angle under the head of the bolt.
Clean the surface to remove dirt, and then in a vacuum water quenching furnace, keep the temperature at 600-900℃ for 1-2 hours, then water-cool, then grind the rod to the standard rod diameter, and then put it into the rolling machine for rounding strengthening.
Put it into the thread rolling machine to make threads; then clean it again to remove the oil stains on the surface; then in a vacuum aging furnace, keep it at 400‑600℃ for 7‑12 hours, and then air-cool it;
Carry out internal flaw detection, spray lubricant on the surface, carry out dimensional and mechanical properties inspection, and package.
7. What is the application of Titanium Flat Head Screws?
Titanium Phillips Screws are used in the petrochemical industry (high-temperature resistance, chemical resistance, corrosion resistance, prolonged the service life of the equipment)
Titanium flat-head bolt is applied in the electronics industry (insulation, anti-interference, lightweight)
Titanium flat head bolt countersink can be used in the communication industry (insulation, non-magnetic, safety)
Flathead Phillips drive titanium screw is used in the shipbuilding industry (acid resistance, alkali resistance, corrosion resistance, prolonging service life), etc.
8. Where to buy the Phillips flathead titanium screws?
Titanium Screw Flat Head has some sizes in stock, we have not only supplied Titanium Phillips Screws but also slotted titanium screws, material various from gr2 to gr12, it can also be ordered according to your drawings, you call us now to buy our titanium screws and send us a mail to get its price, we will be glad to provide you fast and reasonable quotations.
Our China Factory DIN7505 Yellow White Zinc Plated Torx Pozi Phillips Double Csk Flat Head Harden 6X55 3.5X30 MDF Stainless Wood Furniture Chipboard Screw is in the leading position in the same industry in terms of design, development, testing methods, technology and equipment capacity, and quality. Our company has established an effective organizational structure, formulated a reasonable and effective talent system and innovated our marketing channels. Based on our own experience, we are committed to becoming a leading, dedicated and professional excellent company.
Hot Tags: phillips flat head titanium screws, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Molybdenum, small TUNGSTEN crucible, titanium CP Grade 4 sheets, Gr5 Alloy of Titanium Foil Ti 6al 4V Foils, tantalum foil for sale, Titanium Reducer Manufacturers