ASTM F67 Grade12 Alloyed Titanium Plate From China Supplier

ASTM F67 Grade12 Alloyed Titanium Plate From China Supplier

Bt1-00 Titanium Plate
VT1-0 titanium plate
Sheet titanium BT1-0
BT1-0 titanium alloy plate
Send Inquiry
Chat Now
Description

Our company's TUNGSTEN bar stock, titanium clad copper wire, Titanium Flange have been loved by users from all walks of life for many years. Due to the continuous efforts and tireless pursuit of our company, it has been fully affirmed and deeply cared by many authoritative organizations. We have an advanced production team, a mature design team, and a passionate sales team. Our design team is enterprising, innovative and good at planning, which makes the design full of vitality and creativity. Our vision is to become a century old enterprise with responsibility, industry status and sustainable profitability. We will provide the best quality and service to our customers with the highest efficiency. We wish to join hands with all people from all walks of life to create brilliance together!

Products Introduction

1. BT1-0 titanium plate is a Russia-grade titanium sheet metal, which is one of the most widely used pure titanium grades, its corresponding American grade is Gr2.

2. BT1-0 titanium plate available size and standards

OD: 0.3~100mm or the customer's size

Standards: ΓOCT22178-90 ΓOCT23755-87 DIN17860-1990

3. Features of BT1-0 titanium plate

It has the Al element(0.3~0.7) vs Gr2 pure titanium, which is softer and has higher elongation.

Sheet titanium BT1-0
Bt1-00 Titanium Plate

4. What are the chemical compositions of the BT1-0 titanium plate?

GradeChemical composition (mass fraction) (%) is not greater than (except for the specified range value)

TiAlCrMoSnMnVFeSiZrCNHOthe sum of other elements
BT1-0base0.3~0.70.250.10.070.040.010.20.3
Gr2base0.30.080.030.0150.250.4

5. What are the applications of the BT1-0 titanium plate?

BT1-0 titanium plate is used as a titanium electrolytic plate and titanium electrolytic cell in electrolysis and sewage desalination, and as a tower body and kettle body in titanium reaction towers and titanium reactors. It is used as exchangers, reaction towers, synthesizers, autoclaves, etc in industries such as petrochemical, fiber, pulp, fertilizer, electrochemistry, and seawater desalination.

6. Package and delivery

Standards export package: wooden case package or wooden case with steel frame package

10kg or below are wooden pallet packaging

Bt1-00 Titanium Plate manufactures

7. Our advantages

We BT1-0 titanium plate manufacturer in Baoji, are specialized in manufacturing titanium with years of export experience, our products were sold to Asia, Europe, North America, and Korea, All products we produced are based on the standard: German standard, Aerospace standard, European standard, etc, including ANSI/ASTM, JIS, DIN, etc.

8. Where to buy BT1-0 (VT1-0) titanium plate?

Call us to get the BT1-0 Titanium plate price or send us mail at sales@tmsalloy.com for a quotation, we will be glad to talk with you about your inquiries.

We widely participate in international cooperation and hope our ASTM F67 Grade12 Alloyed Titanium Plate From China Supplier and services go to the world. Our company is actively working on the research and development of new products, developing deep processing products with higher technological content, higher added value and better market prospect, and we sincerely welcome people with insight from all sides to come to our group to show their talents. In the future, we will make unremitting efforts, relying on products, and will continue to forge ahead and seek.

Hot Tags: CP titanium Grade 1 GOST-22178 BT1-0 Titanium Plate, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, ECCENTRIC titanium reducer, titanium welding wire price, TUNGSTEN bar for sale, titanium round target, Titanium Reducer, asme pressure vessel heads