With advanced product testing equipment and modern testing methods to ensure that high-quality and competitive nickel crucible temperature, titanium strip suppliers, titanium strip suppliers continue to enter the market. While our industry returns to the society, we are also enthusiastic about public welfare, sincerely repay the society and establish a good corporate image. We pay attention to the growth and personal value of our employees, and shape their personal quality comprehensively.
Products Introduction
1. 3al2.5v titanium tube is an alpha-type titanium alloy tube with a nominal composition of Ti-3Al-2.5V, which is developed as a cold-workable tube application.
2. Basic Information
Ti-3Al-2.5V titanium tubing can be cold worked by standard tube manufacturing processes or supplied in the annealed condition. Other applications include bicycle and wheelchairs frames.
Product Name | 3al2.5v Titanium Tube |
Grade | Gr9 3al2.5v |
Specification | Outer Diameter 6-108.0mm |
Length | <10 000mm |
Wall Thickness | <10 mm |
Standard | ASTM B337 ASTMB338 |
Application | Petroleum Oil Chemical Industry etc |
3. Special Properties Ti Gr 9 pipe
Excellent Resistance to pitting and crevice / erosion-corrosion
High Mechanical strengths, superior to the C. P Titanium Grades
Grade 9 Titanium alloy pipe contains 3.0% Al and 2.5% V. It is the trade-off between the ease of welding and manufacturing of the "pure" and the high strength of the grade.
Detail Shows
Gr9 titanium tube
3al2.5v titanium tube
4. Hydraulic pipelines and sporting goods frequently employ 3al2.5v titanium tubing. In particular in seawater, where it can withstand the high-speed erosion and corrosion of seawater, it has corrosion resistance that other metal materials can't match. In addition, titanium control equipment and devices are widely used in coastal power stations, offshore oil extraction equipment, seawater desalination, marine chemical production, and marine aquaculture.
5. Permissible deviation of the outer diameter of titanium pipe(mm)
OD | 3~10 | >10~30 | >30~50 | >50~80 | >80~100 | >100 |
Tolerance | ±0.15 | ±0.30 | ±0.50 | ±0.65 | ±0.75 | ±0.85 |
In an effort to finest meet up with client's requirements, all of our operations are strictly performed in line with our motto 'High High quality, Competitive Rate, Fast Service' for ASTM B861 Gr2 China Mmm 100 Mmm Titanium Tubing. In order to better serve our customers in all aspects, our company has been investing a lot of manpower and resources to improve the one-stop purchasing experience. With advanced processing equipment, advanced management mode and excellent technical personnel, our company always keeps innovating and forging ahead.
Hot Tags: 3al2.5v Gr9 Seamless Titanium Tube, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, 6mm titanium rod, Grade 5 Titanium Screws, tantalum round target, Tungsten Bar, Titanium Steel Clad Metal, nickel strip roll