As an honest manufacturer, we always use excellent raw materials, advanced equipment, and skilled technicians to ensure that our zirconium plate for sale, zirconium fishing rod, Mo Boats for Evaporation is finished in high quality and with stable characteristics. Relying on our product innovation ability, wholehearted service consciousness, and the integration of advanced operation models, we will surely lead the company to a new round of rapid development! The key to improve the corporate image is to create the core competence of brand competition and cultivate competitive advantage.
1. Zirconium 702 foil is a metal thin coil made of zirconium, which has a min thickness of 0.025mm, wide of around 100mm, it is widely used in the electronic and chemical industries.
2. Size and standards
Thickness: 0.025-1mm
Width: 10 ~ 300mm, length: ≥ 500mm
Standards: ASTMB551


3. What is the manufacturing process of the zirconium 702 foil?
The production process of zirconium foil consists of main processes (hot rolling, cold rolling, multi-roll rolling mill rolling foil) and auxiliary processes (pickling, degreasing, heat treatment, and shearing). The cold-rolled zirconium strip is the original material of rolled foil. The zirconium strip is cold rolled many times after pickling and annealing, and the total deformation of each cold rolling is controlled at 20% ~ 40%. After degreasing and vacuum annealing, we can cut it into strips according to different customer requirements.
4. Chemical elements according to ASTMB551
Element | R60702 |
Zr+haf | 99.2 |
haf | 4.5 |
Fe+Cr | 0.2max |
Tin | ... |
H | 0.005 |
N | 0.025 |
C | 0.05 |
N | ... |
O | 0.16 |
5. What are the applications of zirconium 702 foil?
Zirconium can absorb a large amount of oxygen, hydrogen, ammonia, and other gases during heating, it is an ideal getter. For example, zirconium powder is used as a degassing agent in electronic tubes, and zirconium wire, zirconium sheets, and zirconium foil are used as grid and anode support.
6. Our advantages
We have advanced equipment, rolling process control, annealing temperature, and time control that can effectively avoid the wrinkling phenomenon on the surface of zirconium foil, ensure the flatness and finish, and effectively improve the product quality.
7. Package and delivery
White paper or waterproof film wrapped around, pearl cotton inside and wooden case outside.
We cooperate with international express companies like FedEx, DHL, TNT, etc, air and sea freight are also available, we deliver customers good quality products with a short lead time because we have raw material ready stock and if you buy zirconium 702 foil from us, 3rd party test report also supported, welcome to call us for inquiry.
We are writing a new chapter in the development of the industry with excellent technology and leading ASTM B551zr702 Zirconium Plates in Minerals & Metallurgy. We have always believed that honor only represents the past, and providing you with the best service is the key to our development. We will produce the goods according to your request.
Hot Tags: zirconium 702 foil, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, tantalum foil surgery, Titanium Gr 2 Sheet Plate, Tantalum Alloy Tube Pipe, Titanium Buttweld Reducer, 10mm titanium rod, 6al4v Titanium Rod