Our customers recognize the consistent excellence of our company's Gr5 Titanium Alloy Bar, grade 4 titanium dental implants, TITANIUM GRADE 5 Bar and are always inclined to buy our products. We grasp the development trend of the world economy, with the vision of creating an advanced enterprise with international competitiveness, and strive to achieve scale development. We hope that by strengthening the training of talents in order to enhance the governance and prosperity of the enterprise. We will do our best to serve customers and look forward to achieving cooperation and friendship between both parties.
Products Introduction
1. Gr5 titanium plate also known as Ti6Al4V, Ti-6Al-4V, or Ti 6-4 titanium plate, is the most commonly used alloy.
2. Product information
Titanium plate size: T x W x L (mm)
Thickness (4.1-60.0) x Wide (400-3000) x Length (1000-4000)
Thickness (0.3-4.0) x Wide (400-1500) x Length (1000-3000)
Product surface | Pickling surface, water-polished surface, shiny bright surface |
No cracks, peeling, oxide scale, crushing, alkali washing traces on the surface | |
Product section | Water cutting, shearing cutting, milling surface, laser cutting, wire cutting |
Product raw materials | High-quality titanium sponge ingot |
3. Titanium Gr 5 plate chemical and physical features
Chemical composition:
Grade |
N |
C |
H |
Fe |
O |
Al |
V |
Pa |
Mo |
Ni |
Ti |
Gr 5 |
0.05 |
0.08 |
0.015 |
0.40 |
0.20 |
5.5~6.75 |
3.5~4.5 |
/ |
/ |
/ |
bal |
Tensile properties:
Grade |
Tensile strength(min) |
Yield strength(min) |
Elongation (%) | ||
Ksi |
Ksi |
MPa |
Ksi |
MPa |
|
5 |
130 |
895 |
120 |
828 |
10 |
4. Gr5 titanium plate performance
It has good machining performance and needs to use carbide tools, large cutting volume, slow speed, and sufficient cooling. Good corrosion resistance and good thermal stability. It is suitable for long-term working parts below 400℃.
Detail Shows

6al4v titanium plate

titanium alloy plate
5. What is the application of titanium gr5 plate?
Titanium Grade 5 is found as the most used alloy in many areas.
- Aerospace and Aircraft
- sports equipment
- Medical industry
- chemical Industry

6al4v titanium plate

6al4v titanium block
6. Titanium other applicaitons
Titanium and its alloys are used in the general industry to make electrodes in the electrolysis industry, condensers in power stations, heaters for petroleum refining and seawater desalination, and environmental pollution control devices. Gr5 titanium plates have become a kind of corrosion-resistant structural material. In addition, it is also used in the production of hydrogen storage materials and shape memory alloys.
7. Titanium alloy grade types
There are hundreds of titanium alloys in the world, the most famous are Ti-6Al-4V, Ti-5Al-2.5Sn, Ti-2Al-2.5Zr, and other 20-30 types. 32Mo, Ti-Mo-Ni, Ti-Pd, SP-700, Ti-6242, Ti-10-5-3, Ti-1023, BT9, BT20, IMI829, IMI834, etc.
8. Our Package and Service

titanium sheet

titanium plate

3.0mm titanium plate
9. Our advantages:
We have a large amount of inventory, as a high-quality Gr5 titanium plate supplier, we can provide samples, can be processed and customized according to drawings, and can provide third-party inspection reports.
FAQ
Q: 1. Is grade 5 titanium good?
Q: 2. What is the difference between gr2 and Gr5 titanium plate?
Gr5 titanium plate is often used in aviation engine parts, high-temperature furnaces, and chemical equipment due to its excellent corrosion resistance and high strength.
Price and market supply
Gr2 titanium plate has a relatively low price and sufficient market supply, making it suitable for large-scale production and general industrial applications.
Gr5 titanium plate has a higher price and relatively less market supply and is mainly used in high-end and special application fields.
Gr2 and Gr5 titanium plates differ in composition, performance, and application areas. You can choose the right material according to your specific needs.
Q: 3. Is the Gr5 Titanium Plate in stock?
Q: 4. Can the Gr5 Titanium Plate be cut?
Contact information:
Tel: +86-0917- 3664600
Whatsapp: +8618791798690
Email: sales@tmsalloy.com
tina@tmsalloy.com
Our company's tenet is to meet the market demand in an all-round way with the best quality, the best price and the most complete variety of ASTM B256 Titanium Anode Plate Titanium Cold Rolled Sheet, so as to provide the best value-added service for domestic and foreign users. We will continue to develop, to provide the high-quality products and services, and promote lasting cooperation with our customers and create a better future. We adhere to the people-oriented human resources policy, respect people, cultivate people, treat people well, and establish a fair, just and open working and development environment for employees.
Hot Tags: ASTM B265 UNS R56400 TA6V Gr5 Titanium Plate, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, m2 titanium screws, Grade 2 Titanium Welded Pipe, Molybdenum rivets, 1 8 titanium sheet, ASTM B363 wpt2 Elbow, 5 inch titanium pipe