Over the years, our company has established a scientific management and advanced technical testing team, we rely on excellent equipment and rich production experience to ensure the quality of Molybdenum Screws Fasteners and Fixings, tungsten boat price, 1 lb titanium bar. As one of the leading enterprises in the industry, we actively undertake relevant responsibilities and contribute to the healthy, sustainable and high-level development of the industry. For the environment, we provide strong impetus to the pursuit of sustainable development through industrial transformation and upgrading.
1. Molybdenum fasteners include molybdenum screws, molybdenum bolts, molybdenum nuts, molybdenum washer, etc. The purity is over 99.95%, and the high-temperature resistance can reach over 1600°-1700°. Molybdenum screws are widely used in vacuum furnaces, single-crystal furnaces, LED furnaces, glass ceramics, and other equipment.
2. Mo Fasteners size and standards
Grade: Mo1, TZM
Standard: DIN933, DIN931, DIN85, etc.
Density: 10.2 g/cm3
Purity: 99.95%
Melting point: 2610℃
Working temperature: 1700℃ under vacuum or inert gas
Manufacture process: forging rods -- rolling
3. Features of molybdenum fastener
High-temperature resistance: Molybdenum has a very high melting point, ranking sixth among the elements in nature, and is called a refractory metal. molybdenum bolts still have good physical strength above 1700 degrees
High hardness: the hardness of molybdenum is high, and the Mohs hardness is 5~5.5.
High thermal conductivity: Molybdenum has a very low coefficient of thermal expansion and high thermal conductivity. The resistivity is low.


4. Mo Fastener types
The types of molybdenum screws are divided into round head types, flat head types, and oval head types according to different nail heads. There are two types of slotted screws and cross groove screws on the nail head. Generally, round head screws and flat head screws are polished and oval. Head screws are usually cadmium chrome plated. Specifications are determined by rod diameter, length, and nail head type.
5. What are the applications of Mo Fastener?
Molybdenum fasteners, molybdenum screws, molybdenum bolts, and molybdenum nuts have high-temperature resistance, and corrosion resistance, and are not easy to deform, especially in industrial production applications, such as engineering construction, vacuum furnace, engine equipment, etc. In many environments, production equipment requires high temperature-resistant molybdenum screws, so as to ensure that the equipment will not loosen or fall off at high temperatures.
6. Other applications of Molybdenum
Molybdenum and chromium, nickel, manganese, and silicon can manufacture different types of stainless steel, tool steel, high-speed steel, and alloy steel. The stainless steel made has good corrosion resistance and can be used for corrosion-resistant steel pipes for oil exploration. Stainless steel with about 6% molybdenum can also replace titanium for seawater desalination devices.
7. Why choose us?
We select high-quality raw materials, the processing technology is meticulous, and there is a strict quality control process. Some specifications of molybdenum screws and molybdenum nuts are in stock, and third-party testing is supported. We have a young and energetic team, fast response, providing buyers with high-quality products, cost-effective service is our goal, if you need to buy molybdenum fasteners, please contact us, we will be in the first time to respond and give you a detailed molybdenum screw price and formal quotations.
Our workshop
8. Package and delivery
Packing: standard export wooden box, the weight of a single box does not exceed 200kg
Shipping: Express or logistics to the customer's designation
We provide rich and high quality ASTM A193 B7 B8 B8m Stud Bolts for our customers by increasing our product development efforts. Our company has a good reputation and abundant capital reserve. We are able to provide you with a wide range of high quality hair products at competitive prices.
Hot Tags: High temperature resistance R03600 Molybdenum Fastener, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, zirconium crucible hs code, Anodizing Titanium Disc Rack, 6-4 titanium, Gr.1 Titanium Clad Plate, Titanium Alloy Semi Elliptical Head Dish End, plate titanium