We are specialized in producing titanium mesh screen, nickel wire 0 025 price, Gr2 Titanium Round Bar over many years. We guarantee the best price based on the same quality and service. Customers are the only reason to determine the existence and development of an enterprise, and for our company, satisfying our customers is just our basic bottom line. Our company casts superior management team in complicated internal and external affairs and cultivates unique corporate culture in the working environment of unity and cooperation and harmony. We take the initiative to adapt to the new normal, follow the trend, and have the ambition to reach new heights.
Products Introduction
1. A titanium target is a metal target made of a highly pure titanium plate or bar, which is used for sputtering PVD film preparation.
2. Basic Information
Titanium target shape: Rectangle, Square, Disc, rotary, tube, rod.
Purity (99.5%, 99.995%), ASTM grade 1, ASTM grade 2, TiAl6V4
Standard: ASTM381, ISO 5832/2, JIS H4650, Din 17851
Shape: Discs (Diameter<350mm), thickness=">1mm Rectangle (Length 1800mm, Width 400mm Thickness>1mm Tube ( Rotary target, OD: 20mm~160mm, Thickness: 2-20mm, Length: custom-made OD>160, Thickness >8mm, length<200)
3. Titanium target application: deposited film nitride as Decorate thin film, Deposited film oxidized to TiO2 as a beam splitter or insulator
Detail Show

Titanium Sputtering target

High-purity titanium target
4. Purity is one of the main performance indicators of the titanium target because the purity of the target has a great influence on the performance of the film. However, in practical applications, the purity requirements of the target material are not the same.
5. The multi-arc target for surface engineering (decorative tool)
Product name | purity | density | Coating dominant color | shape | Regular size | Application industry |
Titanium aluminum (TiAl) alloy target | 2N8-4N | 3.6-4.2 | Rose gold/brown | Cylindrical | diameter 60/65/95/100*30/32/40/45mm | Decoration industry |
Pure chromium (Cr) target | 2N7-4N | 7.19 | White/Black | Cylindrical | ||
Pure titanium target (Ti) | 2N8-4N | 4.51 | Golden yellow/gun black | Cylindrical | ||
Blue/rose red | ||||||
Pure zirconium (Zr) target | 2N5-4N | 6.5 | gold | Cylindrical | ||
Pure aluminum (Al)) target | 4N-5N | 2.7 | Silver | Cylindrical | ||
Pure nickel (Ni) target | 3N-4N | 8.9 | Metal color | Cylindrical | ||
Nickel vanadium (Ni) target | 3N | 8.57 | blue-green | Cylindrical | ||
Pure niobium (Nb) target | 3N | 8.57 | White | Cylindrical | ||
Pure Tantalum (Ta) Target | 3N5 | 16.4 | black purple | Cylindrical | ||
Pure molybdenum (Mo) target | 3N5 | 10.2 | black | Cylindrical |
6. Titanium circular targets are a widely used titanium material product, with the main application areas as follows:
Aerospace: Titanium circular targets are highly suitable for use in the aerospace industry due to their lightweight and high-strength properties. For example, in the aerospace field, titanium circular targets can be used to manufacture aircraft, missiles, and rocket components.
Chemistry: Titanium circular targets are not easily corroded, so they can be used to manufacture chemical reactors and other chemical equipment.
Electronics: Due to its excellent conductivity and corrosion resistance, titanium circular targets can be used to manufacture electronic components and circuit boards.
Automotive manufacturing: Titanium circular targets are also used in the automotive manufacturing industry, for example, to manufacture high-performance wheels and other automotive components.
In summary, the characteristics of titanium circular targets are excellent corrosion resistance, high strength, lightweight, and other properties, which have been widely used in many fields.
We will do our best to maintain our reputation in terms of quality and reliability of the ACETRON 99.6% High Purity Ti Rotating Target for Vacuum/PVD Coating, thus building a good corporate image. We insist on serving the needs of customers as the starting and ending point of our work, and creating value for customers as an important focus of our work. Our company is committed to establishing a sound management mechanism with space for development and guaranteed benefits to achieve the harmonious unification of enterprise and employee values.
Hot Tags: Gr1 Round metal target Titanium Target, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, hemispherical tank heads, titanium fittings;, 1 625 titanium tube, titanium bar factory, brushed nickel strips, molybdenum wire price