We have been committed to the development and sales of zirconium rod guides, Wheel bolt Titanium BMW, nickel foil roll at home and abroad. We would appreciate your inquiry and trial order as soon as possible. Our company takes integrity, pragmatism, innovation and development as the concept and zealously serves the vast number of users.
Products Introduction
1. Tantalum tube is a refractory metal pipe, which has extremely high corrosion resistance, and moderate hardness.
2. Basic Information
Tantalum tube grades: R05200, R05400, etc.
Tantalum pipe standard: ASTM B521-98
Purity: The purity of pure tantalum is greater than 99.95%;
State: annealed state (M) or hard state (Y).
3. Tantalum can produce seamless and welded tubes, both of which are often utilized. Seamless pipe is manufactured by extrusion, pipe shrinkage, or deep drawing with a metal plate. The welding manufacturing method is to form the strip first, then make it into a tube shape, and then weld the joint with a gas tungsten arc (GTAW).
Detail Shows

tantalum seamless tube

tantalum round tube
4. Classifications for tantalum tubes
Seamless tantalum tube
-
Able to create capillary materials and tiny pipes
-
Excellent adaptability; suited for creating goods with numerous specifications and small batches.
-
The performance of each part of the pipe is uniform
Generally suitable for the production of small batches of products with many specifications.
Tantalum welded pipe
-
Uniform wall thickness, good internal surface quality, and high production efficiency.
-
High production efficiency. low cost
-
Easy to produce large-diameter pipes
-
Short production cycle
-
Product quality is easy to control
Generally suitable for the production of large batches of products.
5. Tantalum tube Unlike ordinary metals, tantalum cannot be hot processed, The recrystallization temperature of tantalum exceeds 1000 degrees Celsius, and excessive oxidation will occur. More seriously, if tantalum is exposed to such a high temperature, not only the surface of tantalum will be over-oxidized, but also oxygen will be reduced also invade the atoms inside the matrix. In the meantime, the tantalum becomes brittle. Not only oxygen but even nitrogen, carbon, and hydrogen can make tantalum brittle.
Our company has been committed to providing professional services for customers, providing high-quality 2022 Low Price with Good Quality From China Tantalum Tubes Pipe and technical services is our purpose. We need to build a sustainable production and operating system, do fine and excellent brand, bigger and stronger enterprises. The development of any industry is inseparable from talents, who are the source of enterprise development.
Hot Tags: 99.95% Purity Seamless Tantalum Tube, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, MSS SP 43 ASME B16 9, Ti Cu clad bar, gold titanium bolts, strip titanium anodizing, Titanium stainless Clad Steel Plates, Titanium Steel Composite Plate