Ni200 Ni201 Pure Nickel Bar

Ni200 Ni201 Pure Nickel Bar

Pure nickel rod
Ni200 Ni201
3.0~300mm
bright surface
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of ni200 ni201 pure nickel bar in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

Products Description Tel:0917-3664600

Pure nickel bar refers to a solid cylindrical metal form made entirely of nickel with a high degree of purity, it is also known as pure nickel rod. These bars are commonly stock (pure nickel bar stock), and are used in a wide range of applications due to their unique properties.

Product features:

Corrosion Resistance: Pure nickel is highly resistant to corrosion and oxidation, making it ideal for use in harsh environments where other metals would quickly deteriorate.

Heat Resistance: Pure nickel bar has a high melting point and is resistant to extreme temperatures, making it ideal for use in high-temperature applications such as heating elements.

Ductility: Pure nickel rod is ductile and can be easily shaped and formed using various methods such as forging, machining, and welding.

Electrical Conductivity: Pure nickel has excellent electrical conductivity properties, making it ideal for use in electrical applications such as batteries and electronics.

Magnetic Properties: Pure nickel rod is magnetic, making it ideal for use in magnetic applications such as sensors and magnetic storage devices.

Chemical Stability: Pure nickel is chemically stable and does not react with most acids or alkalis, making it ideal for use in chemical processing, pharmaceuticals, and medical devices.

pure nickel bar pure nickel for sale
Specification Tel:0917-3664600
Grade Ni200 Ni201 
Size 6.0~300mm
Surface polishing bright surface
Standards ASTMB160
Factory Tour Tel:0917-3664600
pure nickel bar ni200 ni201
pure nickel rod price
pure nickel bar supplier
 
Composition of pure nickel bars Tel:0917-3664600

The composition of pure nickel bars is typically 99.9% or higher nickel content, with trace amounts of other elements such as iron, copper, and zinc. Due to the high nickel content, these bars are highly resistant to corrosion and oxidation and are also non-magnetic. This makes them ideal for use in industries such as chemical processing, electronics, and aerospace, where corrosion resistance and non-magnetic properties are critical.

Machanical properties of pure nickel rod Tel:0917-3664600

In terms of mechanical properties, pure nickel bars have excellent ductility and a low coefficient of thermal expansion, making them highly resistant to deformation and cracking at high temperatures. They also have a high melting point and are capable of withstanding extreme temperatures, making them ideal for use in high-temperature applications.

Packing And Shipping Tel:0917-3664600

details4-5.jpg

details4-6.jpg

FAQ

Q: 1. What is the density of the pure nickel rod?

A: The density of pure nickel rods is about 8.9g/cm. This value is mentioned in multiple sources, and although there are slight differences (such as 8.99/cm* and 8.902g/cm*), they are all within a similar range and can be considered acceptable errors.

Q: 2. What material is the pure nickel rod made of?

A: Pure nickel rod is a silvery-white metal with excellent corrosion resistance and processing properties. Its density is 8.9g/cm3 and its melting point is 1453℃.
At room temperature, a dense and strong protective film will form on the surface of a pure nickel rod, which makes it have excellent corrosion resistance. In addition, pure nickel also has excellent welding and processing properties and can be processed into products such as tubes, rods, wires, plates, strips, foils, etc.

Q: 3. What is the hardness of the pure nickel rod?

A: The hardness of pure nickel rods is usually between HRB90-95 or HV188-215.
These hardness values ​​are affected by multiple factors, including chemical composition, heat treatment, and work hardening.
For example, the higher the nickel content of pure nickel rods, the lower their hardness; while adding elements such as chromium and molybdenum can increase the hardness of pure nickel rods. In addition, heat treatment can change the grain size and metallographic composition inside pure nickel rods by adjusting temperature and time, thereby affecting its hardness. Excessive work hardening should be avoided as much as possible during the production process to avoid adverse effects on mechanical properties.

Q: 4. Is nickel rods easy to process?

A: Not easy to process. Pure nickel rod is a silvery-white iron family metal. It has a melting point of 1452℃, strong corrosion resistance, a certain strength, good plasticity, and heat resistance, but its machinability is extremely poor. Cutting characteristics The cutting temperature is high and concentrated; the affinity is particularly strong, and it is very easy to bond with elements such as Co, Ni, and Mo in the tool material, so cutting pure nickel with carbide tools will fail due to bonding; pure nickel has good plasticity and difficult chip breaking.

Overall, pure nickel bars are a popular and versatile choice for a variety of industries due to their unique properties and high degree of purity. They are available for sale from a variety of sources and can be used in a wide range of applications due to their corrosion resistance, non-magnetic properties, and high-temperature capabilities.

Other related pure nickel for sale

nickel foil roll

pure nickel wire

Contact information:

Tel: +86-0917- 3664600

Whatsapp: +8618791798690

Email: sales@tmsalloy.com
tina@tmsalloy.com

Hot Tags: ni200 ni201 pure nickel bar, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Nitinol Bar & Rod, Nitinol Shape Memory Bar

Send Inquiry

(0/10)

clearall