Titanium wide and thick plate in stock:
TA1 TA2 TA9 TA10 TA7 Gr1 Gr2 Gr7 Gr12 Gr6 >2000x6000mm
The rolling process method titanium wide and thick plate. Titanium thick plate is based on the raw material of blooming or forging slab, "through the basic production processes such as heating - rolling - hot straightening - heat treatment - interruption - correction - descaling - pickling, and then processed according to the requirements of the surface. If it needs to be polished, it shall be polished with sandcloth" to finally produce the finished thick plate.